Dear All,

We have sub contracted our pipe welding work based on ASME B31.3 and ASME sec IX qualified WPS to another organization. Is it allowed in ASME section IX for a sub contractor to use the main contractor's WPS.

anand gupta

unread,
Oct 6, 2016, 2:22:47 PM10/6/16
to material...@googlegroups.com
Dear 
as per ASME SEC IX you can not use wps of another party.
But another part have give written permission to use wps and your client accepted then you can use the wps.

Regards
a p gupta


On Tue, 4 Oct, 2016 at 18:16, thulaib arakkal
Dear All,

We have sub contracted our pipe welding work based on ASME B31.3 and ASME sec IX qualified WPS to another organization. Is it allowed in ASME section IX for a sub contractor to use the main contractor's WPS.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2L2JMBzSCg4sYKoc2SsFKSEMEQRi-YwMBpOpAnY%3DQM-gH-JQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Hareesh K V

unread,
Oct 6, 2016, 2:22:53 PM10/6/16
to materials-welding

If the subcontractor is approved by the client (The agency which awarded the contract to you) then you can use subcontractor WPS.

The main  contractor WPS can be used by subcontractor as the work is awarded to the main contractor and it is only based on the internal work award system the main contractor have awarded the work to subcontractor and the welding control acticities are with the main contractor only.

Regards,

Hareesh K.V
+91-8547859202

syed moinul hasan

unread,
Oct 7, 2016, 10:30:01 AM10/7/16
to material...@googlegroups.com
No issue indeed, as long as there is a mutual consensus by both party.
Cheers
Syed Moinul Hasan

On 6 October 2016 at 22:00, 'anand gupta' via Materials & Welding <material...@googlegroups.com> wrote:
Dear 
as per ASME SEC IX you can not use wps of another party.
But another part have give written permission to use wps and your client accepted then you can use the wps.

Regards
On Tue, 4 Oct, 2016 at 18:16, thulaib arakkal
Dear All,

We have sub contracted our pipe welding work based on ASME B31.3 and ASME sec IX qualified WPS to another organization. Is it allowed in ASME section IX for a sub contractor to use the main contractor's WPS.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/498559274.9392695.1475776831560%40mail.yahoo.com.

John Henning

unread,
Oct 7, 2016, 1:16:26 PM10/7/16
to material...@googlegroups.com

Sorry guys – incorrect answer. 

 

For ASME B&PV fabrication, WPS’s and PQR’s may not be transferred, given, swapped, or sold between independent companies.  The only situation where another company or subcontractor can use your WPS’s if the other company or subcontractor works solely under the control of your QC program (such as might happen if you hired temporary welders) .  You also need a provision in your quality control program documentation to describe how this is going to implemented.

 

Too many incorrect answers to this one.

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of syed moinul hasan
Sent: Thursday, October 06, 2016 10:18 PM
To: material...@googlegroups.com
Subject: Re: [MW:25497] Usage of ASME Sec 9 WPS for sub contractor

 

No issue indeed, as long as there is a mutual consensus by both party.

Cheers

Syed Moinul Hasan

On 6 October 2016 at 22:00, 'anand gupta' via Materials & Welding <material...@googlegroups.com> wrote:

Dear 

as per ASME SEC IX you can not use wps of another party.

But another part have give written permission to use wps and your client accepted then you can use the wps.

 

Regards

 

On Tue, 4 Oct, 2016 at 18:16, thulaib arakkal

Dear All,

 

We have sub contracted our pipe welding work based on ASME B31.3 and ASME sec IX qualified WPS to another organization. Is it allowed in ASME section IX for a sub contractor to use the main contractor's WPS.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

 

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMXKe_ov-fjWLptrMfprLgj4Voa0WJovB3F6eTuYdNgrjnE3rA%40mail.gmail.com.

Alan Denney

unread,
Oct 9, 2016, 9:26:43 AM10/9/16
to material...@googlegroups.com

Lalu Rajendran

unread,
Oct 9, 2016, 9:27:44 AM10/9/16
to material...@googlegroups.com
Hi,

There is no issue if it is agreed in the contract or specified in the scope of work, as longs as the organisation/company who owns the WPS/PQR doesn't have any issues.

Or you may write a new wps based on this project sub-contractor scope and issue to your sub-con with the existing PQR.

regards,
LALU

On Tue, Oct 4, 2016 at 4:46 PM, thulaib arakkal <thulaib...@gmail.com> wrote:
Dear All,

We have sub contracted our pipe welding work based on ASME B31.3 and ASME sec IX qualified WPS to another organization. Is it allowed in ASME section IX for a sub contractor to use the main contractor's WPS.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

John Henning

unread,
Oct 10, 2016, 10:29:51 AM10/10/16
to material...@googlegroups.com

Not if you are going to be compliant with ASME IX.  This is strictly prohibited.  B31.1 requires qualification in accordance with Sc IX, by the way.  The Code is not giving this up to discussion.  If the contract requires qualification in accordance with Sc IX, WPS’s can only be used as described in my previous reply.

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Lalu Rajendran


Sent: Saturday, October 08, 2016 12:31 AM
To: material...@googlegroups.com

Subject: Re: [MW:25511] Usage of ASME Sec 9 WPS for sub contractor

 

Hi,

 

There is no issue if it is agreed in the contract or specified in the scope of work, as longs as the organisation/company who owns the WPS/PQR doesn't have any issues.

 

Or you may write a new wps based on this project sub-contractor scope and issue to your sub-con with the existing PQR.

 

regards,

LALU

On Tue, Oct 4, 2016 at 4:46 PM, thulaib arakkal <thulaib...@gmail.com> wrote:

Dear All,

 

We have sub contracted our pipe welding work based on ASME B31.3 and ASME sec IX qualified WPS to another organization. Is it allowed in ASME section IX for a sub contractor to use the main contractor's WPS.

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

 

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13sidwLUA%2BKKz%2B%2BYWVhz48bD88r_qeSnmW%3DT4bBhH1o5rg%40mail.gmail.com.

Reply all
Reply to author
Forward
0 new messages