Hardness acceptance

34 views
Skip to first unread message

Saurabh Jain

unread,
Oct 6, 2025, 6:20:35 AM10/6/25
to material...@googlegroups.com
Hello,

Can anyone confirm Hardness acceptance criteria & code requirements for SS to inconnel PQR.

We are following ASTM E92, and considering 310 HV max average, with no single value above 320 HV. 

Is this okay for 316 to 6625 material?


Regards 
Saurabh Jain

Harish Kannepalli

unread,
Oct 6, 2025, 7:38:31 AM10/6/25
to material...@googlegroups.com
Hi Saurabh ji,
     If this pqr is for oil & gas, please follow NACE MR0175 part 3.

Regards,
Mr. Harish.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADr-LL-8tJ%3Dh7mXpdc4_mxEkSzX%3DQm-3N8dB0MWo_2uVZj0L-w%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages