LIMIT OF WELDER QUALIFICATION OVER DIA. RANGE

1,141 views
Skip to first unread message

shailesh dave

unread,
Aug 13, 2008, 4:11:02 AM8/13/08
to material...@googlegroups.com
DEAR MEMBERS,
 
I HAVE COME ACROSS AN INTERESTING SITUATION.
 
WE HAVE WELDERS QUALIFIED IN 6" x 7.11 mm THK. PIPE OFF COURSE BUTT WELD. MY QUESTION IS CAN THESE WELDER PERFORM WELDING OF SMALL BORE PIPE LIKE 3/4" SOCKET WELD.
 
PL. HELP ME.
 
REGARDS,
 
S.N.DAVE
 
QA/QC INCHARGE
ADGAS, DAS ISLAND, UAE

SENTHILKUMAR SWAMINATHAN

unread,
Aug 13, 2008, 6:00:07 AM8/13/08
to material...@googlegroups.com
Refer:  ASME Sec 9, Page 143

GROOVE-WELD DIAMETER LIMITS
(See notes 1,2)
                                                                                                                        
Outside Diameter Outside Diameter Qualified, in.
of Test Coupon, in. Min. Max.
                                                                                                                        
Less than 1 Size welded Unlimited
1 to less than 2 7 /8 1 Unlimited
2 7 /8 and over 2 7 /8 Unlimited
                                                                                                                        
NOTES:
(1) Type and number of tests required shall be in accordance with QW-452.1.
(2) 2 7 /8 in. O.D. is the equivalent of NPS 2 1 /2 .
 
Regards,
S.Senthilkumar

--- On Wed, 13/8/08, shailesh dave <snd...@yahoo.com> wrote:


Unlimited freedom, unlimited storage. Get it now

carloso...@terra.com

unread,
Aug 13, 2008, 10:47:05 AM8/13/08
to material...@googlegroups.com
YES, YOU CAN TO WELD  ALL FILLET WELD, BECAUSE BUTTWELD QUALIFY ALL FILLET, ASME IX PAR QW-452



On Wed 13/08/08 06:00 , SENTHILKUMAR SWAMINATHAN skuma...@yahoo.co.in sent:
Refer:  ASME Sec 9, Page 143

GROOVE-WELD DIAMETER LIMITS
(See notes 1,2)
                                                                                                                        
Outside Diameter Outside Diameter Qualified, in.
of Test Coupon, in. Min. Max.
                                                                                                                        
Less than 1 Size welded Unlimited
1 to less than 2 7 /8 1 Unlimited
2 7 /8 and over 2 7 /8 Unlimited
                                                                                                                        
NOTES:
(1) Type and number of tests required shall be in accordance with QW-452.1.
(2) 2 7 /8 in. O.D. is the equivalent of NPS 2 1 /2 .
 
Regards,

S.Senthilkumar

--- On Wed, 13/8/08, shailesh dave wrote:

romio dabre

unread,
Aug 14, 2008, 7:40:09 AM8/14/08
to material...@googlegroups.com
please write the code? As per ASME sec IX it is not allowed

shailesh dave

unread,
Aug 14, 2008, 11:17:55 PM8/14/08
to material...@googlegroups.com
Dear Romio,
 
It is ASME SEC. IX.
 
Regards,
 
S.N.Dave

--- On Thu, 8/14/08, romio dabre <romio...@gmail.com> wrote:
From: romio dabre <romio...@gmail.com>
Subject: [MW:1032] Re: LIMIT OF WELDER QUALIFICATION OVER DIA. RANGE
To: material...@googlegroups.com

carloso...@terra.com

unread,
Aug 15, 2008, 9:04:20 AM8/15/08
to material...@googlegroups.com


Yes, the welders can to weld all fillet welds because , if  your qualification was buttweld(groove-joint)

carloso...@terra.com




On Thu 14/08/08 07:40 , "romio dabre" romio...@gmail.com sent:

babu raghavan

unread,
Aug 20, 2008, 11:39:55 AM8/20/08
to material...@googlegroups.com
Mr: S.N.DAVE CHECK ASME SECTION IX  QW 451.4.You can see the details.This welder can weld 3/4 " socket weld.
 
BABU.P.R
 


--- On Fri, 8/15/08, shailesh dave <snd...@yahoo.com> wrote:

alireza alavi

unread,
Aug 21, 2008, 5:48:27 AM8/21/08
to material...@googlegroups.com

Dear My freinds ,
 
I need some information , references on the web or code for " double wall isolateted vaccum tanks "  for storage of nitrogen liquid or some things like that such as oxygen , argon ,.....
 
Best regards
Alavi

Message has been deleted

shabbir ahmad

unread,
Aug 22, 2008, 5:54:32 AM8/22/08
to material...@googlegroups.com
Dear Dave
 
Babu n carlos are right, u can weld any fillet, in any diameter as per QW451.1 if you have qualification as per /qw451.1 n qw 451.2.
 
You can weld in short
 
Shabbir

Binit Kumar

unread,
Dec 18, 2018, 9:16:26 PM12/18/18
to Materials & Welding
Dear Friend,
As per code ,Joint Design- Any Groove,Pipe Diameter-Any,Pipe Thickness-Any.So he qualified any diameter and thickness of fillet weld.


Regards,
Binit Kumar