Dear members,
We are going to carry out a Mockup Procedure qualification for T-TS joint as per ASME SecIX. what are the test required to carry for the qualification. I hear from a TPI that RT, Tear test & pull out has to be carried out, whereas ASME Sec IX & Tema class 'R' are not talking about the above said tests. 
Is the above said tests required? If so, the as per which standard?
Kindly advice

BR,
M.V.Silambarasan

Mohd Azam

unread,
Jan 12, 2015, 2:36:01 AM1/12/15
to material...@googlegroups.com

ASME SEC IX will tell only PT and Maco Examination is to be done, If you have as per ASME SEC IX than it’s not required. Client spec. will speak about (Pull out, Tear Test etc.) these test, Pls check if you have any client specification applicable.

 

Thanks & Regards,

Mohd. Azam


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eb910586-77a2-4489-a880-880f18dbb748%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Saravanan Sornam

unread,
Jan 12, 2015, 2:36:11 AM1/12/15
to material...@googlegroups.com
Hi Silambarasan ,

If the welding is for ASME Sec VIII Div -1 Vessel, then test Macro ( for MLP check ) , PT, Visual. This is enough as per ASME-IX QW - 193 requirements.

Hardness & RT are Special Tests as per Client requirements only, inorder to judge the hardness value . Quite Stringent too.

Pull out & Tear tests are required for Sec VIII , Div-2 Vessels, If I am not mistaken.

Do you have Client Spec to weld this MockUp ?

Read again ASME-IX,  QW 193. 1 to 3 for MockUp testing requirements and you must read QW-288 for Essential Variables to follow during Qualification.

Regards,
Saravanan

 

--

Saravanan Sornam

unread,
Jan 12, 2015, 3:32:05 AM1/12/15
to material...@googlegroups.com
Hi Mohd,

ASME Sec-IX, QW-193.1.1, Visual Examination is also must.

See all the Acceptance Criterias given.

Regards,
Saravanan

Thiyanes Kowshi

unread,
Aug 1, 2015, 6:04:52 AM8/1/15
to Materials & Welding
 Dear  Members,
 
I had a doubt about TTS joint mockup pullout test , as per the configuration no welding only expnansion , let me know the fr. value for that.
 
Best regards 
 