PWHT for fillet welds ASME B 31.3

188 views
Skip to first unread message

Ilkin Hasanov

unread,
Jun 12, 2020, 6:20:46 AM6/12/20
to material...@googlegroups.com
Hi Gents 
Could you please advise are there any requirements for PWHT of fillet welds asper ASME B 31.3 ?


Regards, 
Ilkin Hasanov

pradip kumar Sil

unread,
Jun 18, 2020, 7:01:02 AM6/18/20
to materials-welding
Which Material

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDYy1_AmnHNMtBWM48rpC827G52WPSFvyt7SUwg%3D3%2BOy6g%40mail.gmail.com.

Ilkin Hasanov

unread,
Jun 18, 2020, 10:03:13 AM6/18/20
to material...@googlegroups.com

luis carlos greggianin

unread,
Jun 18, 2020, 10:03:13 AM6/18/20
to material...@googlegroups.com
Ilkin, the criteria requirements ASME B 31.3 ED 2018
 fillet weld: the throat 

image.png
image.png

--

ishwar kumar

unread,
Jun 18, 2020, 10:03:42 AM6/18/20
to material...@googlegroups.com
Plz see to it for better understanding of fillet welds PWHT requirements 


Thanks & Regards
Ishwar Kumar
IWE CSWIP 3.1 NDT LEVEL II
ISGEC HEAVY ENGINEERING LTD.
+91 8758806284,8930111584

--
IMG_20200618_172742_Burst01.jpg

Raja Varman

unread,
Jun 19, 2020, 10:55:33 AM6/19/20
to material...@googlegroups.com
Based on throat thickness the requirements applicable.
Please refer ASME B31.3 Table 331.1.1 and
Exemption is Table 331.1.3


என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584