Can i weld A36 or equivalent S275JR with E7018-B2L?

50 views
Skip to first unread message

chris

unread,
Apr 12, 2020, 11:46:46 PM4/12/20
to Materials & Welding
our customer specifies ultra low carbon content with elevated nickel. Is there any other welding that i can use in this case?

james gerald

unread,
Apr 13, 2020, 12:56:40 AM4/13/20
to material...@googlegroups.com
What is your MDMT (minimum Design Metal temperature) at which Impact test to be conducted.

Try E 7018-C3L as it provides Impact test upto to -50degC and also contains Nickel.

E 7018-B2L is a chromium Molybdenum electrode which do not contain much Nickel

Thanks & Regards

J.Gerald Jayakumar



On Monday, April 13, 2020, 10:46:39 AM GMT+7, chris <chris...@gmail.com> wrote:


our customer specifies ultra low carbon content with elevated nickel. Is there any other welding that i can use in this case?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f52cfb16-c52a-436a-a0af-7437a3aa51c8%40googlegroups.com.

Chris Sabu

unread,
Apr 13, 2020, 8:17:52 AM4/13/20
to material...@googlegroups.com
hi james,

They really don't have any impact test requirement which is weird though. They require carbon content less than .04% and elevated nickel content.
I don't see any variation with both these parameters.




--
THANKS AND REGARDS
CHRIS SABU
0559695451

George Dilintas

unread,
Apr 13, 2020, 8:17:55 AM4/13/20
to material...@googlegroups.com
You should look on SFA-5.5

Στις Δευ, 13 Απρ 2020 στις 6:46 π.μ., ο/η chris <chris...@gmail.com> έγραψε:
our customer specifies ultra low carbon content with elevated nickel. Is there any other welding that i can use in this case?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f52cfb16-c52a-436a-a0af-7437a3aa51c8%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

james gerald

unread,
Apr 14, 2020, 12:08:50 AM4/14/20
to material...@googlegroups.com
From the Material ASTM A36 and 275JR I understand they are not LTCS material.

try E 7018C2L or E 7018C1L with the maximum carbon of 0.05% and welding consumable MTC will show lower amounts.

Inline image

It also depends on the number of Joints you intend to weld,

Thanks & Regards

J.Gerald Jayakumar




Kannayeram Gnanapandithan

unread,
Apr 14, 2020, 1:08:46 AM4/14/20
to materials-welding
7018-1 itself will work for-43°C

Chris Sabu

unread,
Apr 14, 2020, 3:36:21 AM4/14/20
to material...@googlegroups.com
Thanks James ,
I think I can work something out with this


Reply all
Reply to author
Forward
0 new messages