why do we use dollymix welding technique in pipelines?

1,756 views
Skip to first unread message

aslam khan

unread,
Aug 11, 2010, 1:41:19 PM8/11/10
to material...@googlegroups.com
dear all ,
i want to know why do we use dollymix welding technique in pipelines?thanks

pirama rayan

unread,
Aug 15, 2010, 2:19:13 AM8/15/10
to material...@googlegroups.com
Dear Mr.Khan,
 
To minimise the Heat Input,we are using Dollymix welding Technique.
 
Thanks.
 
Piramaryan B
Welding Engineer -CSWIP SCWI 3.2.2
ILF CONSULING ENGIEERS (PMC) KSA

 
On Wed, Aug 11, 2010 at 8:41 PM, aslam khan <aslam...@gmail.com> wrote:
dear all ,
i want to know  why do we use dollymix welding technique in pipelines?thanks

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

IMRAN KHAN

unread,
Aug 15, 2010, 3:19:11 AM8/15/10
to material...@googlegroups.com
DEAR
        Mr.Pirama rayan
 
kindly explain me
1-how heat input will be minimise in dollymix technique in pipeline?
2-for what purpose we are using this method?
 
by
KHAN
ksa
 



 



--- On Sun, 15/8/10, pirama rayan <piram...@gmail.com> wrote:

pirama rayan

unread,
Aug 15, 2010, 3:36:24 AM8/15/10
to material...@googlegroups.com
Mr.Khan
 
As you know , Dollymix Technique means combination of use of both uphill and downhill progression during welding.
 
If you use Uphill Progression alone ,there will be high heat input for lower thichness pipelines .That's why we use this technique.
 
Hope you cleared now.
 
thanks.
 