Dear All

We need to conduct Face bend and Root bend test for AA 6061-T6,  P.No.23 as per ASME Sec IX.

Thickness of PQR test coupon is 10mm.

We have machined face bend and Root bend specimens with following dimensions  - 300mm L × 38mm wide × 10mm Thick.

Can anyone explain what will be the Test jig / Mandrel dia. as per ASME Sec IX , QW 466.1.
For eg. In steels it is 4T.

Regards

Prem Nautiyal

rishikesh shahi

unread,
Jun 3, 2021, 8:27:48 AM6/3/21
to material...@googlegroups.com
Dear Team,

I have to Weld IS 2062 PLATE,  E 550 GRADE BR Plate.

Please suggest welding Consumable for SMAW, GMAW and SAW welding Wire...


Its Urgent..

Regargs.
Rishikesh Shahi 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEP2HKA%3DOBtRN612TD-kaMHXtEyNZB72-g-qVigdXXLa2bWc6A%40mail.gmail.com.

james gerald

unread,
Jun 3, 2021, 10:12:11 PM6/3/21
to material...@googlegroups.com
Dear Mr. Prem,

I suppose the thickness will be 3mm for P23 as per below snap shot.


Inline image

Thanks & Regards

J.Gerald Jayakumar




Vishwas Keskar

unread,
Jun 3, 2021, 10:12:11 PM6/3/21
to material...@googlegroups.com
 AA 6061-T6,  P.No.23 as per ASME Sec IX.
Pl. inform  % elongation of this material .

Vishwas Keskar

unread,
Jun 3, 2021, 10:12:11 PM6/3/21
to material...@googlegroups.com
I suggest - 
Pl. consider wrap around jig shown in Figure QW-466.3 due to less  elongation of these materials   

On Thu, Jun 3, 2021 at 5:26 PM Prem Nautiyal <prem.na...@gmail.com> wrote:

james gerald

unread,
Jun 3, 2021, 11:24:00 PM6/3/21
to 'james gerald' via Materials & Welding
Just to add,

I suppose the bend specimen dimension may be as 150mm x 3mm x 10mm

Thanks & Regards

J.Gerald Jayakumar