Dear all, can some help me with ASEM equivalent of EN 10025-2-S355JR

KajaASW

unread,
Oct 20, 2010, 6:50:29 AM10/20/10
to material...@googlegroups.com

 

ASTM equivalent of EN 10025-2-S355JR  is ASTM A572 GR.50

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

RAJAGOPAL KANNAN

unread,
Oct 21, 2010, 4:25:46 AM10/21/10
to material...@googlegroups.com
Dear All,
I have a doubt in the statement below.
ASTM A572 Gr. 50- Not necessarily hot rolled fine grain, yield is 330N/Sq. mm
S355JR - Hot rolled fine grain steel, Yield is 355 N/Sq.mm
How then these two or equivalent?
Thanks,
K.Rajagopal

Karthik

unread,
Oct 21, 2010, 11:59:38 PM10/21/10
to material...@googlegroups.com
Hi,
There is no exact equivalent material for S355JR in ASME or ASTM.There are some equivalent in other standards are below.
 
S355JR equivalent to BS4360 - 50B/50C and DIN17100-St52-3.
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Thu, 10/21/10, RAJAGOPAL KANNAN <rajagopa...@gmail.com> wrote:

Navid Navidi

unread,
Oct 21, 2010, 12:41:18 AM10/21/10
to material...@googlegroups.com
please find attached file.


From: KajaASW <ka...@asw.com.sa>
To: material...@googlegroups.com
Sent: Wed, October 20, 2010 2:20:29 PM
Subject: [MW:7663] RE: 7650] ASEM equivalent of EN 1025 S355JR
S355.pdf
Reply all
Reply to author
Forward
0 new messages