i have some doubts in WPS, if possible kindly clarify me

1) If PQR is done with Normalization heat treatment (PWHT done above the upper critical temperature), what is the qualified base metal thickness range to be taken ( min to max ) any special condition applicable in ASME Sec IX?

2) When Impact test is applicable to the WPS, then what is the qualified base metal thickness range to be taken ( min to max ). any special condition in ASME Sec IX?

Vishwas Keskar

unread,
Aug 15, 2021, 11:57:20 PM8/15/21
to material...@googlegroups.com
Let us know what  is P NO of  PQR ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0e6d52d2-c48a-4159-bf6f-88511b0a5ff6n%40googlegroups.com.

Sourav Bohrays

unread,
Aug 16, 2021, 7:40:33 AM8/16/21
to material...@googlegroups.com
1. No restriction for thickness ( Qw 451.1)
2.refer qw 403.6


Best regards
Sourav 



--

mohit aggarwal

unread,
Aug 16, 2021, 7:40:33 AM8/16/21
to Materials & Welding
IF PQR is done with Normalization heat treatment then the same thk range will apply as per table QW 451.1

and  when Impact test is applicable to the WPS then depend on the thickness of base metal then following clause will apply
code, standard, or specification.
QW-403.6 The minimum base metal thickness qualified
is the thickness of the test coupon T or 5/8 in.
(16 mm), whichever is less. However, where T is 1/4 in.
(6 mm) or less, the minimum thickness qualified is 1/2T.
This variable does not apply for any of the following
conditions:
(a) WPS is qualified with a heat treatment above the
upper transformation temperature.
(b) WPS is for welding austenitic or P-10H material and
is qualified with a solution heat treatment.
(c) Base metals are assigned to P-No. 8, P-Nos. 21
through 26, and P-Nos. 41 through 49.

Regards,
Mohit Aggarwal.

sangram routray

unread,
Aug 16, 2021, 7:40:35 AM8/16/21
to Materials & Welding
Dear Mr. Pandiyan

please Mention the thickness of PQR.
Accordingly any one can say you MIN & MAX limit.
for Impact test Follow QW 403.6 

Thanks & Regards

Sangramkeshari Routaray
Zeeco India,
Cswip3.1, NDT level-II (UT,RT,MT & PT)
ISO Lead Auditor 9001:2015



--

Raja

unread,
Aug 17, 2021, 11:24:18 PM8/17/21
to Materials & Welding
Dear sir,
pl refer the details,
Base metal Thk is 50mm, and P-Number is 15E (Gr.91 material)

sangram routray

unread,
Aug 18, 2021, 1:17:36 AM8/18/21
to Materials & Welding
Dear Mr. Pandiyan 
please  find below attached for without Impact test.(5-200mm) QW451.1
for impact tested range will be also same see below attached detail QW403.6
Inline image

Inline image

Thanks & Regards

Sangramkeshari Routaray
Zeeco India,
Cswip3.1, NDT level-II (UT,RT,MT & PT)
ISO Lead Auditor 9001:2015

james gerald

unread,
Aug 18, 2021, 2:44:24 AM8/18/21
to material...@googlegroups.com
I doubt where do you get this requirement of Normalizing either during Hot Forming or Hot pressing. For P15E (Gr.91 material), Tempering below AC1 is mandatory after Normalizing for P15E materials. Hence QW451.1 thickness criteria apply  performing final heat treatment below lower critical temperature.

Some snap shots below from ASME Sec. VIII Div.I

Inline image


Inline image


Some snap shots from Material standard IIA

Inline image


Inline image


Thanks & Regards

J.Gerald Jayakumar



Ganesh Muthurajan

unread,
Aug 19, 2021, 12:17:55 AM8/19/21
to material...@googlegroups.com
change in thicknes andtemp range is in essential variable

thicknes range qualified as per QW 450.2


Regards

M. Ganesh