RE: SSPC SP 6 - 63

155 views
Skip to first unread message

pgos...@rogers.com

unread,
Nov 26, 2020, 10:51:16 AM11/26/20
to RKD, material...@googlegroups.com

Hi,

I think there’re some mix-ups in the specifications and interpretations. SSPC SP6 or other specifications are applicable for  surface preparation by blasting for application of paints.

For the refractories the criteria is a bit different. Following is the extract from  API -936, for surface preparation before applications of refractory.

You may read the standard, discuss and settle the issue with the client based on the API-936 guidelines.

Thanks.

 

 

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

From: RKD <raymondkenn...@gmail.com>
Sent: November 26, 2020 10:15 AM
To: Materials & Welding <material...@googlegroups.com>
Subject: SSPC SP 6 - 63

 

Hello everyone.

 

I encountered a requirement from a Licensor specification that internal surface should be prepared as per SSPC SP 6 - 63 prior to refractory application.

 

I know SSPC SP 6 means commercial blast but I have never encountered or saw a surface preparation requirement "SP 6 - 63".

 

Does anyone know what this means?

 

Thank you in advance.


Virus-free. www.avg.com
image003.png

RKD

unread,
Nov 26, 2020, 10:14:17 PM11/26/20
to Materials & Welding

RKD

unread,
Nov 30, 2020, 5:00:34 AM11/30/20
to Materials & Welding
Hi Sir,

Thank you for your valuable input. Indeed we have to discuss with Client and Licensor about this requirement. Normally we just do the SP-7 as specified in API 936 but we would need to install acid coating that would require a more clean surface so it would not peel-off. Thus we may need to clarify with the Refractory Supplier about the required acid coating and its required surface preparation before we talk to Client/Licensor. 