Impact test at -210 Deg C

30 views
Skip to first unread message

chiluka venkatramulu

unread,
May 25, 2019, 1:44:06 AM5/25/19
to material...@googlegroups.com
Dear All,
Anybody know the mechanical labs, who can conduct impact at -210 Deg C in India.

Thanks & Regards,
Venkatramlu.C

anand gupta

unread,
May 25, 2019, 5:03:43 AM5/25/19
to material...@googlegroups.com, chiluka venkatramulu
Check met heat engg. 
Vadodara Gujarat  india. 

They have facilities to do impact at - 210 deg c. 

Regards 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdGH4d4JqvdjFKb6sPFfo2bp4NFpA09MBYG3%3DUngPZb4qg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

anand gupta

unread,
May 27, 2019, 12:02:14 PM5/27/19
to ramulu...@gmail.com, material...@googlegroups.com
Sir

For which material reqd. Impact at - 210.
I think every body have facilities upto - 196 only. 
Re check your requirements and procede. 

Regards 
A p gupta 
ThyssenKrupp 
QC manager 
Baroda 
On Mon, 27 May 2019 at 15:09, chiluka venkatramulu
Dear Mr.Guptha,
Thank you for your information. But I enquired with them, they are conducting impact up to -196 Deg C only. Pl let me know if any other labs are there.

Thanks & Regards,m
Venkatramulu C

amit singh

unread,
Jun 1, 2019, 12:58:47 PM6/1/19
to material...@googlegroups.com
Dear Sir,
Please check with Exova metallurgical Lab, Mumbai.

Regards,
Amit Singh

Reply all
Reply to author
Forward
0 new messages