welding A335 P91 with Carbon steel

392 views
Skip to first unread message

mauricio padilla

unread,
Jun 6, 2010, 5:31:13 PM6/6/10
to material...@googlegroups.com
Sirs,
 
I have a question about welding dissimilar material:
 
One Metal:          A335 P91 ----------------------------------        PNumber 15E
Second Metal      MSS SP75 WPHY-70  ---------------        Snumber 1
 
Wall thickness                                                              36.53 mm
 
Which ones are the best  FILLER METAL for   GTAW?
 
Which ones are the best  FILLER METAL for   SMAW?
 
 
Is it necessary PWHT?
 
Please give a tips.
 
Best Regards
 
Mauricio

Prabhu Kumar L

unread,
Jun 7, 2010, 3:12:31 AM6/7/10
to material...@googlegroups.com

Dear Mauricio,

 

Please provide code of construction.

 

In general ASTM A335 P91 requires PWHT for all thickness. For more detail, specify the code of construction and application.

 

For filler material, it is suggested to use E9018-B9 (SFA 5.5) for SMAW & ER90S-B9 (SFA 5.28) for GTAW processes. Both the filler materials shall meet the minimum yield and tensile strength of WPHY-70.

 

Precautions such as preheating of 250ºC and post heating of 300ºC for ½ to 1 hour would reduce problems related to hydrogen induced cracking. After post heating, PWHT shall be carried out in accordance with design code.

 

Regards,

 

L. Prabhu kumar,

Sr. Principal Engineer,

 

Equipments & Materials Dept.,

Saipem India Projects Limited,

Nungambakkam High Road, Chennai - 600 034, India.

Tel:+91 44 43906588, Ext.: 588, Fax:+91 44 66840345,

Mobile Ph. No.: +91 9003010978.


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

 




-------------------------------------------------------------------------------------------------------------------------------------------------------------------
DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or 
entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged 
information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution 
or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If 
you have received this communication in error, please notify us immediately by responding to this email and then 
delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete 
transmission of the information contained in this communication nor for any delay in its receipt. 
-------------------------------------------------------------------------------------------------------------------------------------------------------------------

AGUSTIN JIMENEZ

unread,
Jun 7, 2010, 9:00:52 AM6/7/10
to material...@googlegroups.com
Hello Mauricio.
Looking for a electrode with similar element that the metal with more element and afther other PQR similar.
Review ASME IX and API 1104.
 
Agustin
 


De: mauricio padilla <mauricio_...@yahoo.com>
Para: material...@googlegroups.com
Enviado: dom, junio 6, 2010 5:01:13 PM
Asunto: [MW:5416] welding A335 P91 with Carbon steel

mahendra reddy

unread,
Jun 9, 2010, 12:50:42 AM6/9/10
to material...@googlegroups.com
Dear Mauricio
 
As per my Knowledge best Filelr wire to use : ER 90S-B9 for GTAW
 
E9015-B9 FOR SMAW.
 
RGDS
M.M.REDDY
QA/QC INSPECTOR (MECHANICAL)
METHANOL PLANT
DAMIATTA - EGYPT
0020168194532



 
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Reply all
Reply to author
Forward
0 new messages