Welding consumable testing requirements are always as per ASME Sec II, Pt-C. See the extracts on the testing requirements for E-6010 electrodes. E-7010 electrodes are covered under SFA 5.5. Usually welding qualification codes e.g., Sec-IX deals with welding procedure & performance qualifications only. Welding consumables have to be tested or the Certificate of Conformance is to be issued by consumable manufacturer, not by the fabricator.
Hope this clarifies your query.
Thanks.
Pradip Goswami.P.Eng, IWE.
Independent & Consulting Welding & Metallurgical Specialist
Saudi Aramco Approved Designated Welding Engineer(DPWR)
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@rogers.com,pradip....@gmail.com
Cell/Whasapp:1-905-9793232

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPv03Fv-jN_dXtQ_%2BwhBcDR-gtFH77_VJTOMmfNxod-t838DTQ%40mail.gmail.com.