Mechanical test for Welder qualification

170 views
Skip to first unread message

Muhammed Ibrahim PK

unread,
Jan 30, 2019, 9:34:05 PM1/30/19
to material...@googlegroups.com
Gents,

Is it mandatory mechanical test qualification for welders as per ASME B31.8 sour gas service requirement as per clause B823.2?.

Qualification by RT is acceptable ?.

image.png
Thanks & Regards
Muhammed Ibrahim PK

munee...@gmail.com

unread,
Jan 31, 2019, 8:20:14 AM1/31/19
to materials-welding
Hi,

As per B801 clause ''provisions apply'' does not seems to be your case as 823.2  / B823.2 both para exists simaltaneously, also as per below interpretation 13-7-Q4, sour gas service can be qualified as per IX of ASME for procedure, to be noted again it is very clearly written ''if a weld procedure for sour gas service is qualified under asme IX'' where as when we come B821.4 it stipulates weld acceptance as ASME IX  which is qualification too?  anyhow as per this interpretation when it is ensured procedure qualified under IX then you can go also for performance and snatch your qw-304 alternatives regardless of B823.2.

Note: File 03-154, interpretation 13-7-Q4 is just reference for the subject and i would like to know more experts interpretations.

Thanks.



Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
munee...@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Catch.jpg
image(01-31-12-11-22).png

Ramin Kondori

unread,
Feb 2, 2019, 2:17:55 AM2/2/19
to material...@googlegroups.com
Because it is a repeated work, pipeline standards ask for DT and it is a right thing to do.
It is highly recommended to follow this method of qualification.
RT is not as effective as DT for screening good welders in pipeline projects.

Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


--

Muhammed Ibrahim PK

unread,
Feb 2, 2019, 2:27:58 AM2/2/19
to material...@googlegroups.com
Hi, 

Can we accept the welders as per RT qualification?. If mechanical test omitted will be it violation of B31.8?.

Reg,
Ibrahim

munee...@gmail.com

unread,
Feb 6, 2019, 12:08:34 AM2/6/19
to materials-welding
Ibrahim,

If you are proceeding after the fact and want to elude from the requirements use my below clause.

or i agree with Mr.Ramin go for destructive which will be before the fact and proactive side.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
munee...@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
image(02-06-10-11-27).png

PRASANTH RAJAN

unread,
Nov 4, 2019, 10:15:03 PM11/4/19
to material...@googlegroups.com
So we have to all the destructive test as mentioned in Api 1104 section 5.4??????

Pls confirm 

--

Bathula AnilKumar

unread,
Nov 4, 2019, 10:40:29 PM11/4/19
to material...@googlegroups.com

For Sour Gas Service Destructive testing is must


​Regards,
 
Bathula AnilKumar
Engineer ‑ Quality Assurance (Mech)
Oil & Gas
Email: bathula....@alturki.com
Mobile: +968 99351283
CPN: 1873
From: material...@googlegroups.com <material...@googlegroups.com> On Behalf Of PRASANTH RAJAN
Sent: Monday, November 4, 2019 7:52 PM
To: material...@googlegroups.com
Subject: Re: [MW:30205] Mechanical test for Welder qualification

Reply all
Reply to author
Forward