Request for clarification about fixing the round bar.

73 views
Skip to first unread message

Guraicharan Maity

unread,
Oct 31, 2024, 3:50:00 AM10/31/24
to material...@googlegroups.com
Respected Sir,

Tank shell plate is A516 Gr.60 thk above 12.5 mm insulated tank. Can I fix a 6 mm round bar for LRB fixing in the tank shell? What can I use the electrode for fixing the 6 mm round bar? Please help me.


Thanks & Regards,


G C MAITY

+91-8670586777/7908324242/8116375630

Vinay

unread,
Nov 2, 2024, 2:55:20 AM11/2/24
to material...@googlegroups.com
But why the round strip?? There is no restriction on the plate as an insulation attachment....

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKTwAA3wtugS2%3DJu4H3_YMmjh9%3DfV1o0XpNygmb%3DDrp%3DDXbfrw%40mail.gmail.com.

VIVEK DUBEY

unread,
Nov 2, 2024, 3:05:02 AM11/2/24
to material...@googlegroups.com

Yes, you can fix a 6 mm round bar for LRB (Lifting Ring Bracket) fixing in the tank shell made of A516 Gr.60, provided the thickness is above 12.5 mm.

For welding the round bar, you can use low hydrogen electrodes such as E7018 or E7015. These electrodes provide excellent mechanical properties and a low-hydrogen weld deposit, which helps prevent hydrogen-induced cracking.


Guraicharan Maity

unread,
Nov 2, 2024, 4:24:15 AM11/2/24
to material...@googlegroups.com
Respected Sir,

LRB means LRB mattress.