Section VIII Div. 2 vessel repair

344 views
Skip to first unread message

David Stevenson

unread,
Jan 11, 2012, 5:51:57 PM1/11/12
to material...@googlegroups.com

To the experts,

The vessel is a transportation portable tank built under the ASME section VIII div. 2 guidelines, if the shell is damaged and would need to be sectioned or repaired by welding or hot work what documentation and approvals would a repair facility be required to hold in order to make an ASME / NBIC repair that would keep the tank in service as an ASME vessel?

 

I am aware the shop would need an R stamp to repair a Section VIII Div. 1 tank would it be the same for Div. 2?

The tank vessels are of P460NL1 material and others are of SA612 N.

 

Description: cid:_1_0600CFAC0600CD40002C9083C12578D4THE FIRST CHOICE IN TANK CONTAINERS

DAVID STEVENSON
TECHNICAL MANAGER
Eurotainer U.S. INC.
5810 Wilson Rd. Suite 200, Humble, Texas, 77396 USA
Phone 01 832 300 5019 (Direct)● Mobile 01 713 805 0192 ● Fax 01 832 300 5050

email: dstev...@usa.eurotainer.com ● website: www.eurotainer.com

Description: cid:_1_0600E23C0600DFD0002C9083C12578D4 Please consider the environment before printing this document

 

image001.gif
image003.jpg

Pieper QSI

unread,
Jan 12, 2012, 9:02:28 AM1/12/12
to material...@googlegroups.com

Dear Sir,

 

Be aware that both P460NL1 and SA612N are fine grain high strength steels for moderate and low temperature service, so I would not suggest hot working because this will lower materials mechanical properties. If necessary you need to simulate the heat treatment and execute mechanical testing in order to ensure the material keeps its properties.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

--
To post to this group, send email to
material...@googlegroups.com
To unsubscribe from this group, send email to
materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

image001.gif
image002.jpg

pgoswami

unread,
Jan 12, 2012, 10:44:40 PM1/12/12
to material...@googlegroups.com
Hi David,
 
It's mandatory that repair shall be performed by an organization holding "R" stamp.
 
Additionally you may look in the recommendations of API-510 or NBIC. If the service application is for refinery or petrochemicals, then API-510 should be followed
 
API-510 , clause 8.1.1,requirements are as follows:-
  • Repair organization should hold NBIC- R stamp.One holding such credentials may do repair and alterations in both DIV-1& DIV-2 vessels
  • Authorization for alterations to pressure vessels that comply with ASME Section VIII, Divisions 1 and 2, and for repairs to pressure vessels that comply with ASME Section VIII, Division 2, may not be given until an engineer (a P.E) has also authorized the work.

  • Welding procedures shall be thoroughly qualified to meet all DIV-2 requirements.

  • If the vessel was subjected to PWHT during original construction and the repair is deemed to be done without further PWHT, then a Temper bead repair procedure shall be established  as per ASME Sec-IX and additionally as per the guidelines of NBIC-RB or API-510. .

NBIC, Part-3(repair and alteration), clause 3.3.5 addresses requirements for repair in DIV-2 & DIV-3 vessels. The requirements are similar to API-510. Repair  shall be documented in NBIC Form R-1,REPORT Of REPAIR (clause 5.13.1).

API-510,Appendix-A provides the exemption categories for containers and pressure vessels.

If the vessel to be repaired belongs to any of these categories,NBIC guidelines should be followed.

Thanks.

 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Pieper QSI
Sent: Thursday, January 12, 2012 9:02 AM
To: material...@googlegroups.com
Subject: [MW:13461] RE: 13458] Section VIII Div. 2 vessel repair

image001.gif
image002.jpg
Reply all
Reply to author
Forward
0 new messages