316Ti material - GTAW rod selection

144 views
Skip to first unread message

PARAI Reaction Channel

unread,
Jul 5, 2023, 2:34:28 AM7/5/23
to material...@googlegroups.com
Dear Sirs,

Please guide for the selection of GTAW welding rod to weld SS 316Ti pipe shell.

Can we use ER318, as I searched in Google?

Please  confirm and also advise for any special wedding parameters,  shield and purge gas requirements for this welding. 

Regards, 
Saravanan Sornam, 
ANSAN city,
S. KOREA. 

james gerald

unread,
Jul 5, 2023, 3:54:21 AM7/5/23
to material...@googlegroups.com
ER 318 can be used as a Filler rod GTAW for welding  SS316TI

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkLnsNfMo1QaCUR2UVB6dPLRA2gp29xoeDiU4B0N33-W-g%40mail.gmail.com.

Vishwas Keskar Welding Manager WELDING

unread,
Jul 5, 2023, 3:54:25 AM7/5/23
to Materials & Welding
ER318 is a compatible filler metal 

Thanks

Vishwas - IWE 
International Welding Engineer

james gerald

unread,
Jul 5, 2023, 4:13:47 AM7/5/23
to 'james gerald' via Materials & Welding
Shielding & purging gas : ARGON

Thanks & Regards

J.Gerald Jayakumar


PARAI Reaction Channel

unread,
Jul 5, 2023, 11:01:13 PM7/5/23
to material...@googlegroups.com
Good morning Sirs,

Thank you for your reply for my query.

Could you please explain,  why this class ER318 is suitable to weld 316Ti. 

Please provide any link for my knowledge. 

Regards,
Saravanan Sornam, 
ANSAN, 
S.KOREA. 

james gerald

unread,
Jul 6, 2023, 2:13:31 AM7/6/23
to material...@googlegroups.com
SS316Ti  contains Titanium which forms Titanium carbide and thus prevents Intergranular cracking in SS, the composition of ER318 is similar to SS 316 except with the addition of Niobium (columbium) which forms Niobium carbide and provides the stabilization effect and prevents Intergranular cracking.

Thanks & Regards

J.Gerald Jayakumar


james gerald

unread,
Jul 6, 2023, 2:23:20 AM7/6/23
to 'james gerald' via Materials & Welding
Titanium and Niobium provide the same effect But Titanium forms carbide at high temperatures and sometimes it may not form carbide also Titanium containing SS GTAW Filler rod can be used with an inert shielding gas but due to the above problem, it is always preferable to use Niobium containing SS Filler rod.

Thanks & Regards

J.Gerald Jayakumar


Vishwas Keskar Welding Manager WELDING

unread,
Jul 7, 2023, 6:47:26 AM7/7/23
to Materials & Welding
Nb or  Ti , both  form preferential carbide Nb carbide or Ti carbide respectively  than Chromium .
In turn Cr depletion possibility is reduced to the extent of none. Intergranular corrosion resistance is improved.

ER318  chemical composition is similar to TYP 316 with addition of Ti 

thanks 

Vishwas - IWE