WELD DISTANCE AS PER ASME-

850 views
Skip to first unread message

Raneesh.PK

unread,
Dec 9, 2016, 10:35:45 PM12/9/16
to material...@googlegroups.com
Dear experts,

Can any one please confirm the Minimum distance between butt weld joint as per ASME B31.1.

Regards,


RANEESH.PK

QA/QC-WELDING


BEC

syahrul husin

unread,
Jan 16, 2017, 10:46:29 AM1/16/17
to Materials & Welding


Dear Raneesh,

i m not an expert.But i m sure the allowable distance between the weld would be 4T or 50mm.

George Dilintas

unread,
Jan 17, 2017, 3:58:00 AM1/17/17
to Meghanadh K
tHERE IS NO RESTRICTION IN THIS CODE SECTION.
HOWEVER, YOU HAVE TO CONSIDER METALLURGICAL ISSUES.
ONCE MORE, CODE IS NOT AN ENGINEERING HANDBOOK

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ced9223d-c87f-487d-a6fe-764bb18aff69%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

pavan kumar reddy Juturu

unread,
Jan 17, 2017, 6:00:32 AM1/17/17
to material...@googlegroups.com

Dear Raneesh,

The distance between adjacent butt welds is 1D. If not it is never closer than 1 1/2" . This is supposedly to prevent the overlap of HAZs. Min. Spacing of circumferential welds between centerlines shall not be less than 4 times the pipe wall thickness or 25 mm which ever is greater.

Himan Nikdin

unread,
Jan 17, 2017, 7:53:00 AM1/17/17
to material...@googlegroups.com
Dear Raneesh
Would you please introduce your reference?

Sent from my iPhone
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO4WkWkzWpUxvgcKvEh4EHC7%2B7LvmXAnGtkBuo2L3ATaJFchSg%40mail.gmail.com.

cd murali

unread,
Jan 26, 2017, 1:38:51 AM1/26/17
to material...@googlegroups.com
The minimum distance between parallel butt welds shall be 20 mm or three times the wall thickness of the joint, whichever is greater as per Saudi Aramco Standard

Regards


C.D.Mural
i
 
| QA/QC 
​Welding/Piping Inspector
| M.S. Al-Suwaidi Industrial Services Company Ltd| Rabigh Phase-II Petrochemical Project (G.S.T), AR-4501|




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

Kannayeram Gnanapandithan

unread,
Jan 26, 2017, 2:23:12 AM1/26/17
to materials-welding

Weld toe to toe is around ,13mm


On 26-Jan-2017 12:12 pm, "cd murali" <cdmur...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (cdmur...@gmail.com) Add cleanup rule | More info

The minimum distance between parallel butt welds shall be 20 mm or three times the wall thickness of the joint, whichever is greater as per Saudi Aramco Standard

Regards


C.D.Mural
i
 
| QA/QC 
​Welding/Piping Inspector
| M.S. Al-Suwaidi Industrial Services Company Ltd| Rabigh Phase-II Petrochemical Project (G.S.T), AR-4501|




On Sat, Dec 10, 2016 at 6:28 AM, Raneesh.PK <pkra...@gmail.com> wrote:

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGRQ%2BmXZ3%3DqAKgPuTe8UsghXfEdiwt1A11WWZQeYoJqhK%3D0TSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

George Dilintas

unread,
Jan 26, 2017, 5:21:23 AM1/26/17
to Meghanadh K
There is no limitation on B31.1
There is a limitation in PCC-2 but this is applicable for repairs


For more options, visit https://groups.google.com/d/optout.



--

Sikhandar Ummer

unread,
Jan 26, 2017, 10:36:18 AM1/26/17
to material...@googlegroups.com
Please let me know reference STD no.

Sikhandar

Mohd Siraj

unread,
Mar 8, 2017, 5:17:19 AM3/8/17
to Materials & Welding
There is no ref in 31.1