FCAW FILLER WIRE FOR S460M/ ASTM A572 GR 65

27 views
Skip to first unread message

Tajuddin Mohammed

unread,
Feb 2, 2026, 1:25:10 AMFeb 2
to material...@googlegroups.com
Dear All,

Please kindly advise which FCAW, SMAW filler wire/electrode need for welding of S460M

image.png

image.png


--
Thanks & Regards
Mohammed Tajuddin
WELDING INSPECTOR CSWIP 3.1
Contact  0530833486
JUBAIL

Saleem Manhappulath

unread,
Feb 2, 2026, 2:01:06 AMFeb 2
to material...@googlegroups.com
Dear Mr. Thajuddhin

we can use  E81T1-Ni1 for FCAW and  E8018-G for SMAW 

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACZrEUaJAsEZ-Mq3SDeNgU%2BesORe7zdou_Ewgi11L6gTF8ZUnQ%40mail.gmail.com.

james gerald

unread,
Feb 2, 2026, 4:47:54 AMFeb 2
to material...@googlegroups.com
SMAW  -  E8018C1           SFA-5.5
FCAW   -  E81T1-Ni1        SFA-5.28

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



james gerald

unread,
Feb 2, 2026, 4:56:19 AMFeb 2
to 'james gerald' via Materials & Welding
Sorry try

SMAW  E8018C3

Thanks & Regards

J.Gerald Jayakumar