Dear Experts,

I am need of your help , i have got blind flange fabricated from plate selection chart from this forum but difficult to prove to client can you please give me code reference or derived formula.

Your Earliest Response is highly appreciated.

Thanks and Regards,

Yasir


rudolf saldanha

unread,
Apr 14, 2013, 12:48:26 AM4/14/13
to material...@googlegroups.com

hi, the attached file was contributed by one of the members, Check it out.But am afraid, there is no reference to any code as such.


From: Yasir Bhatti <meloy...@gmail.com>
To: material...@googlegroups.com
Sent: Saturday, 13 April 2013, 23:19
Subject: [MW:17365] Non Standard Blind Flange (Fabricated from Plate)

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


Blind flange thickness.pdf

Arunachalam A

unread,
Apr 13, 2013, 2:11:17 PM4/13/13
to material...@googlegroups.com


On 13 April 2013 22:03, Arunachalam A <arun...@gmail.com> wrote:
You can refer ASME Section VIII Div 1- UG 34 for calculating blind thickness.

arun


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Arunachalam.A,



--
Arunachalam.A,

Arunachalam A

unread,
Apr 13, 2013, 2:03:30 PM4/13/13
to material...@googlegroups.com
You can refer ASME Section VIII Div 1- UG 34 for calculating blind thickness.

arun
On 13 April 2013 19:19, Yasir Bhatti <meloy...@gmail.com> wrote:

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Arunachalam.A,

Yane

unread,
May 29, 2018, 10:52:16 PM5/29/18
to Materials & Welding

SPACER & BLIND Thickness Calculation for Internal Pressure (ASME B 31.3)


SPACER & BLIND  Thickness Calculation  for Internal Pressure (ASME B 31.3)
******************************************************************

Step1: Select the Spacer & Blind Material
--------------------------------------------------------------------------------------------------------
Step2: List Down

      Ø  Pipe Outside Diameter, (mm) = D
   Ø  Internal Design Pressure,(Kg/cm²) = P   
   Ø  Design Temperature, (C°) = T

For the material under consideration.
--------------------------------------------------------------------------------------------------------

Step 3: List down

Ø  Allowable Stress, (Kg/cm²)  = S

ASME B 31.3 @ Design Temperature.  (TABLE A-1)
--------------------------------------------------------------------------------------------------------

Step 4: Select

Ø  Joint Efficiency factor = E             (TABLE A-1A)


ASME B 31.3  (TABLE-1A)
--------------------------------------------------------------------------------------------------------

Step 5: Select

Ø  Corrosion Allowance, (mm) = c
--------------------------------------------------------------------------------------------------------

Step 6: Formula @ ASME B 31.3 

                                 3*P
tm   =    dg * √  (--------------)     +  c
                              16*S*E

tm= Calculated thickness including corrosion Allowance, (mm).
dg = Inside Dia. of gasket for RF/FF flanges or gasket pitch dia. for RTJ flanges, (mm).
--------------------------------------------------------------------------------------------------------

Step 7: Compare thickness

If      t > tm

t = Thickness as per API 590

Then selected thickness of Spacer & Blind is OK,
Else revise the thickness.