Dear Sirs,

I have inquiries regarding the comprehension of interpass temperature in ASME :

  1. 1)What code reference is used to ascertain the maximum interpass temperature?
  2. 2)What code reference is employed to establish the interpass temperature for dissimilar welds, such as CS to SS welds?

Kannayeram Gnanapandithan

unread,
Nov 24, 2023, 10:34:22 AM11/24/23
to materials-welding
asme sec 1

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6c2f3530-e9f7-4d0f-a51f-40f799445bdbn%40googlegroups.com.

duybien.com

unread,
Dec 18, 2023, 3:51:20 AM12/18/23
to Materials & Welding
minimize C delusion, max. inter-pass should be 150 for SS x CS.