Fw- Tack welder quailification as per AWS D1.1

202 views
Skip to first unread message

anthony chundal

unread,
Nov 14, 2016, 2:25:43 AM11/14/16
to material...@googlegroups.com
Dear All,

Kindly advice with regards to qualifying tack welders as per AWS D1.1, 

Please let me know about tack welder qualification, its not in ASME, but in AWS it states, whether we can use plate thk of 6mm T joint and weld 50mm length of 6mm size and break the same to check the fusion , is it ok
Inline image 1Thanks and regards,
Anthony.

c sridhar

unread,
Nov 14, 2016, 10:33:47 PM11/14/16
to material...@googlegroups.com
Or, you can qualify a tack welder with a groove joint in 1G and check the root penetration. 



From: anthony chundal <anthony...@gmail.com>
To: material...@googlegroups.com
Sent: Monday, 14 November 2016 12:35 PM
Subject: [MW:25690] Fw- Tack welder quailification as per AWS D1.1

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp-nUO7i4FubD5WAMFmuFT8Kr8ydY%3DKozcwcEBB%2BDqgk%2BA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


anthony chundal

unread,
Nov 15, 2016, 5:06:01 AM11/15/16
to material...@googlegroups.com
Please advice whether i can use 6mm thk plate ,T joint with 50mm fillet weld of 6mm size and break the same to check fusion.

On Tue, Nov 15, 2016 at 7:12 AM, 'c sridhar' via Materials & Welding <material...@googlegroups.com> wrote:
Or, you can qualify a tack welder with a groove joint in 1G and check the root penetration. 



From: anthony chundal <anthony...@gmail.com>
Sent: Monday, 14 November 2016 12:35 PM
Subject: [MW:25690] Fw- Tack welder quailification as per AWS D1.1
Dear All,

Kindly advice with regards to qualifying tack welders as per AWS D1.1, 

Please let me know about tack welder qualification, its not in ASME, but in AWS it states, whether we can use plate thk of 6mm T joint and weld 50mm length of 6mm size and break the same to check the fusion , is it ok
Inline image 1Thanks and regards,
Anthony.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.