Hi,
Please find below my suggestions as marked in RED.
Question.
1.) Can i write WPS range qualify to backing gouging CJP double V or Single V butt joint.? - PQR with ceramic backing or with back gouging qualifies for with back gouging or backing only. For this question answer is qualify for CJP Double V only. not qualified for single V (without back gouging)
2.) And, if i have PQR qualified with back gouging, Can i write WPS range qualify with ceramic backing or not.? - Yes. with back gouging also qualify for with backing.
Thanks & Regards,
(Karthik)
Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8,
Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Hand Phone: 0066 892512282