Can please advice what is the meaning for SUS Material and what's are the heat treatment procedures. Attached details below.
Thanks in advance


From 
Ganesh  
WhatsApp Image 2024-06-28 at 18.06.31.jpeg

Siva

unread,
Jun 30, 2024, 11:01:11 PM (2 days ago) Jun 30
to material...@googlegroups.com

SUS304 (SUS meaning Steel Use Stainless) stainless steel austenite is typically known as the Japanese name for SS304 or AISI 304.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5bd7bc34-c172-422a-a7a2-28ad941e1566n%40googlegroups.com.

Laxmi Industries

unread,
Jun 30, 2024, 11:01:11 PM (2 days ago) Jun 30
to material...@googlegroups.com
Dear Ganesh, 
SUS304 (SUS meaning Steel Use Stainless) stainless steel austenite is typically known as the Japanese name for SS304 or AISI 304. The main difference between the two materials is not any physical property or feature, but how it is referenced in American and Japanese grades.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5bd7bc34-c172-422a-a7a2-28ad941e1566n%40googlegroups.com.


--
  
Anil Batawal
(Production Department) 
+91_9130053430
Pranit Chaudhari.
(Quality Control Engineer)
 +91_9359531288
LAXMI INDUSTRIES,
Gat No. 1539, Sonawane Wasti, Chikhali- Pune- 412114 
laxmi...@gmail.comlaxmi...@gmail.com .
khushal...@gmail.com.

Marcel Paredes

unread,
Jun 30, 2024, 11:01:11 PM (2 days ago) Jun 30
to material...@googlegroups.com
SUS es la primera letra de "Steel Use Stainless" escrita en inglés. El número de acero inoxidable consta de tres dígitos, la serie 300 es acero inoxidable austenítico y la serie 400 es acero inoxidable ferrítico o martensítico.



--

mce mce

unread,
Jun 30, 2024, 11:01:12 PM (2 days ago) Jun 30
to material...@googlegroups.com
Stainless steel is the alloy of chromium and nickel. Sometimes, it is referred as SUS

--

Parminder Singh

unread,
Jun 30, 2024, 11:01:12 PM (2 days ago) Jun 30
to material...@googlegroups.com
SUS is steel use Stainless ..... 