Dish End Spin Hole Block

已查看 65 次
跳至第一个未读帖子

Rahul Chaudhari

未读,
2021年12月26日 11:47:242021/12/26
收件人 material...@googlegroups.com
Dear All, 
Greetings.

WE have manufactured 10% torispherical dish end in house & block dish ends spin hole as per attached photographs. 
Please kindly advise me, is it acceptable as per good engineering practice or not?
Material IS IS2062. Thickness is 10mm. Job - horizontal storage tank


Thanks & Regards,

Rahul Chaudhari
+918149199922
IMG_20211225_141620.jpg
IMG_20211225_141750.jpg

Chiranjeevi A

未读,
2021年12月26日 13:19:382021/12/26
收件人 material...@googlegroups.com
Dear Rahul,

Not acceptable

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V9Dy0ZrYO60YQkbyXXwHaNkqB8AkXreW-ZM_fc75oqVBA%40mail.gmail.com.

Vishwas Keskar

未读,
2021年12月27日 02:26:282021/12/27
收件人 material...@googlegroups.com
What was joint design?
Is that joint is made full penetration ?
What NDT was followed ?

Pl send details 

--

sushil gaur

未读,
2021年12月27日 02:26:282021/12/27
收件人 material...@googlegroups.com
Hole is accepted as per ASME sec viii. But you have to make "v" On hole and than patch. Also patch should be radiography examination.. 

Thanks & Regards
Sushil Gaur. 
M. No. 9530278378

--