Overcoming distortion in SS 304L pressure vessel

74 views
Skip to first unread message

Shahil Saini

unread,
Jan 20, 2021, 10:13:54 PM1/20/21
to material...@googlegroups.com
Hello everyone, 

How to overcome the distortion in pressure vessel of material SS 304L?, having thickness 8mm of two dish-end and shell having thickness of 6 mm, I am attaching photographs of vessel for your reference,



IMG_20210111_154352281.jpg

Jamie Reyes

unread,
Jan 20, 2021, 10:19:26 PM1/20/21
to material...@googlegroups.com
Heat input and weld sequence. Monitor both extensively!

On Wed, Jan 20, 2021 at 7:13 PM Shahil Saini <sainis...@gmail.com> wrote:
Hello everyone, 

How to overcome the distortion in pressure vessel of material SS 304L?, having thickness 8mm of two dish-end and shell having thickness of 6 mm, I am attaching photographs of vessel for your reference,



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_931zTtSjSuhEit%3Dc-5afiAF3nAzqXgUU%3DK53y2oG6A_Q%40mail.gmail.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

Ajay Gupta

unread,
Jan 20, 2021, 11:12:13 PM1/20/21
to material...@googlegroups.com
Hi
You can also use water jet opposite side during welding to control distortion in SS304 L and proper stiffening due to lesser thickness.

Regards
Ajay Gupta




On Thu, Jan 21, 2021 at 8:43 AM Shahil Saini <sainis...@gmail.com> wrote:
Hello everyone, 

How to overcome the distortion in pressure vessel of material SS 304L?, having thickness 8mm of two dish-end and shell having thickness of 6 mm, I am attaching photographs of vessel for your reference,



Shahil Saini

unread,
Jan 24, 2021, 8:39:45 AM1/24/21
to material...@googlegroups.com
Sir, in Repair job of pressure vessel how should we rectify the distortion problem? The figures are given below of the repair job of SS 304L.

IMG_20210120_123127473.jpg
IMG_20210120_123106188.jpg
IMG_20210120_123110733.jpg

Harshad Somani

unread,
Jan 24, 2021, 10:42:53 PM1/24/21
to material...@googlegroups.com
Use Double operator GTAW  ie two welders welding from either side simultaneously in 3G, pulling same weld puddle with Square butt joint,  5 mm gap.
Welders to practice first in 1 M long test plate. Use 2 or -2.4dia filler. 80/120 amps. 
Provide stiffnars to act gap closing . 1stStriking arc welder to add filler in joint gap second welder to operate at lower current level and add filler as and when required moving arc behind 3-4 mm from first welder. His arc also provide argon  shielding to weld  

On Thu, Jan 21, 2021, 08:43 Shahil Saini <sainis...@gmail.com> wrote:
Hello everyone, 

How to overcome the distortion in pressure vessel of material SS 304L?, having thickness 8mm of two dish-end and shell having thickness of 6 mm, I am attaching photographs of vessel for your reference,



Reply all
Reply to author
Forward
0 new messages