Dear Members,
We qualify our WPS on Single V Butt joint design, my concern is that can we use this WPS for fillet welding too.
As per API 1104 SECTION 5.7, 5.8 describing about Fillet weld welding requirement.
Regards,
Waqas Suleman
MW
unread,
Jun 17, 2016, 12:34:06 AM6/17/16
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
yes, A major change in joint design constitutes an essential variable. (although it's vaguedefinition in API 1104, it considers all set in/set on etc. are fillet welds)