We qualify our WPS on Single V Butt joint design, my concern is that can we use this WPS for fillet welding too.
As per API 1104 SECTION 5.7, 5.8 describing about Fillet weld welding requirement.

Regards,

Waqas Suleman

MW

unread,
Jun 17, 2016, 12:34:06 AM6/17/16
to Materials & Welding
yes, A major change in joint design constitutes an essential variable. (although it's  vague definition in API 1104, it considers all set in/set on etc. are fillet welds) 