FILLER WIRE & ELECTRODE USE FOR A 333 Gr6 To A333 Gr6 , A 333 Gr6 To A106 Gr.B

964 views
Skip to first unread message

PRABHUDAYAL MAHTO

unread,
Jun 12, 2023, 11:11:49 PM6/12/23
to material...@googlegroups.com
Dear all,

what is filler wire & Electrode use for  

Pipe material  - A 333 Gr6 To A333 Gr6  and    A 333 Gr6 To A106 Gr.B 


Thanks,

PRABHU  DAYAL 

+919566721541


Dinesh

unread,
Jun 13, 2023, 12:38:07 AM6/13/23
to material...@googlegroups.com
SMAW-e7018-1
GTAW-ER70s-G

Thanks & Regards 


Dinesh Baskaran 




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFbohSc1MwP0gq%2B%2BZt79JQgmmvv_XCXzNM0EyG0UjxvPzHvf2w%40mail.gmail.com.

Pham Thanh Tinh

unread,
Jun 13, 2023, 1:25:08 AM6/13/23
to material...@googlegroups.com
You can use ER80S-Ni1  & E7018-1

Vào Th 3, 13 thg 6, 2023 vào lúc 06:11 PRABHUDAYAL MAHTO <massadmn...@gmail.com> đã viết:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFbohSc1MwP0gq%2B%2BZt79JQgmmvv_XCXzNM0EyG0UjxvPzHvf2w%40mail.gmail.com.


--
Best & Regard
Pham Thanh Tinh
QC Manager
China National Chemical Engineering Third Co.LTD
South Ghawar Gas Separation Plant & Associated Facilities Project
Mobile phone +966. 556802308 


Mubashir khan

unread,
Jun 13, 2023, 7:19:19 AM6/13/23
to material...@googlegroups.com
Yes in our project we are using  ER80S-Ni1 & E7018-1 in Aramco project

Ritesh Kumar Singh

unread,
Jun 13, 2023, 7:29:54 AM6/13/23
to material...@googlegroups.com
Dear all 
Why we can't use Er70S2(spl) & E7018-1 ?

On Tue, 13 Jun 2023, 4:49 PM Mubashir khan <mubashir...@gmail.com> wrote:
Yes in our project we are using  ER80S-Ni1 & E7018-1 in Aramco project

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Dinesh

unread,
Jun 14, 2023, 12:17:20 AM6/14/23
to material...@googlegroups.com
Dear , 

from my understanding..  you mentioned consumable too can use , its all based on base metal tensile strength requirement regarding ..

Thanks & Regards 


Dinesh Baskaran 