ph & Chloride Value for hydro test Water For Cs & SS Materials

2,307 views
Skip to first unread message

Nandush Sreekumar

unread,
Nov 5, 2020, 10:34:02 PM11/5/20
to Materials & Welding
what is the Commonly Recommend ph & Chloride Value for  hydro test Water For Cs & SS Materials 









NANDUSH.S

QC INSPECTOR

MKG GLOBAL LLC

DUQM REFINERY PROJECT-OMAN

MOBILE:968-79614049

Vishwas Keskar

unread,
Nov 6, 2020, 10:43:07 PM11/6/20
to material...@googlegroups.com
No code specified these values.
It is specified in specification.
Generally for SS , it is less than 50ppm

Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e36293e0-a596-4488-a2b9-4c4ee5c3c2c4n%40googlegroups.com.

Bien.ND |WIC

unread,
Nov 11, 2020, 10:45:43 PM11/11/20
to Materials & Welding
Hello,

Here are our procedure, you may refer to it.

Test medium

Test medium shall be cleaned or potable fresh water or rust inhibitor. Note that chloride content in water shall be less than 250 ppm for carbon steel components and chloride content in water shall be less than 50 ppm for stainless steel components.

Regards

Bien ND


Patel Ankit

unread,
Nov 14, 2020, 12:22:34 AM11/14/20
to material...@googlegroups.com
Dear Nandush,

Code dose not specified PH value for Hydro Test.
Pl. Ask to client and Testing according.

Regards,
Ankit Patel
QCE
 Chem Process system private Limited

--

Bien.ND |WIC

unread,
Nov 14, 2020, 9:15:07 AM11/14/20
to Materials & Welding
Yes, code may not required, but project specification may require in the test package. I hope that everyone check in the specification also.

MRTEJS1

unread,
Nov 19, 2020, 10:05:15 PM11/19/20
to material...@googlegroups.com
Dear 

PH & PPM 

1 . C. S - less then 250ppm or specified by client spec. 
2. S.S- 50 ppm Or specified by client spec. 
3. PH - 07 natural water 6.5-7.5 best

Lesser PH value more acidic below 06 Or equivalent 06 for stainless steels, it's better to refer client specifications for PH value


Tejas

--

George Dilintas

unread,
Nov 20, 2020, 11:07:29 AM11/20/20
to material...@googlegroups.com
ASME BPVC has a useful info in Section V - II-641, II-642, II-643

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e36293e0-a596-4488-a2b9-4c4ee5c3c2c4n%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis