Re: [MW:14731] Pipe to Flange welding as per ASME Code

81 views
Skip to first unread message

Chetan Kapadia

unread,
Jul 1, 2012, 6:32:21 AM7/1/12
to material...@googlegroups.com
Dear J.D.Silva,

The simple answer is YES.

It is the weld thk. at joint is taken as consideration by code.
 
Best Regards,
C.B.KAPADIA



From: jdsilva <nithind...@gmail.com>
To: material...@googlegroups.com
Sent: Sunday, 1 July 2012 12:52 AM
Subject: [MW:14731] Pipe to Flange welding as per ASME Code

Dear All,

i have confusion regarding the base material thickness qualified or limit. for eg. consider neck to flange welding. my PQR is qualified to weld 5mm to 24mm. but some portion of the flange like self reinforced hub, has thickness above 50mm. In the portion where bevel is done and welding involved has only 10.97mm. Can i weld this flange with the above PQR?
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


c sridhar

unread,
Jul 1, 2012, 10:45:45 AM7/1/12
to material...@googlegroups.com
Mr. Silva,
You have not  mentioned type of material to be welded. Pl. refer to QW- 202.4 of the Sec. IX ASME code. It says,

WPS qualified on groove joints is applicable for dissimilar thicknesses provided,

a. thickness of the thinner member shall be within the range permitted by QW-451.
b. thickness of thicker member is more than 6 mm or greater if the material is as per the details
    mentioned (like P8, P41, P42  etc.) there in.
c. If it is P1, P11, P22 (other than above P nos) etc., thickness of thicker member within the range
    as permitted by QW 451.
d. More than one PQR may be required for certain thickness combinations.
e. In your case the thickness of the weld joint bevel is 10.97 mm  and do  not require an additional 
    PQR and you can do the welding.

sridhar.