Hi Forum Members,

 

I’ve  come across many companies who perform heat treatments on a regular basis and perform in-house certification of heat treatment technicians. This may incorporate in house theoretical training on various PWHT  followed by field experiences and hand on training.

 

AWS D-10.10  (Clause 14) Recommended  practices for Local  PWHT  insists that operators should be trained and a proper documentation shall be maintained. Equipments used for local PWHT shall be periodically calibrated, such as thermocouples, strip Chart recorders and the heating devices.   

 

Within  our organization, companies performing PWHT are required to show their competence, as and when required.

 

The following documents provide useful information on training of heat treatment technicians:-

 

·          http://www.tradesecrets.gov.ab.ca/occupations/pdf/occupation_exams/209_exams/209_exam_t1.pdf

 

·         http://www.tradesecrets.gov.ab.ca/occupations/pdf/occupation_competency_profiles/209_competency_profile.pdf

 

 

These guidelines specified in these documents may not be mandatory in many places, but training always improves the competence levels and often this may be done in-house.

 

Thanks

 

Pradip Goswami,P.Eng.
Welding & Metallurgical Engineer/Specialist
Component Integrity Section.
Engineering and Training Services
Ontario Power Generation Inc.
Res:-88,Garth Trails Crescent
Hamilton,Ontario, L9B2X1,Canada
 
 

---------------------------- Original Message ----------------------------

Subject: Re: [MW:4740] PWHT Technician'sTraining Requirements

From:    "Declan Foley" <declan...@eircom.net>

Date:    Wed, April 7, 2010 9:07 am

To:      material...@googlegroups.com

--------------------------------------------------------------------------

 

Subramani,

 

I have dealt with a lot of PWHT guys down the years, there doesn't appear to be any formal system of qualification. The majority of them I

know are however trained electricians and the rest just have on the job training......

 

Declan

 

On 07/04/2010 09:03, subr...@batelco.com.bh wrote:

> Is there any reference specifications/standards or guidelines related to

> training and qualifying PWHT technicians.In the absence of above how to

> document their training/qualifications.

> 

> Subramani.

> 

> --------------------------------------------------------------------

> mail2web - Check your email from the web at

> http://link.mail2web.com/mail2web

> 

> 

> 

 

--

To post to this group, send email to material...@googlegroups.com

To unsubscribe from this group, send email to

materials-weld...@googlegroups.com

For more options, visit this group's bolg at

http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and

meant for educational purposes only, Users must take their own decisions

w.r.t. applicable code/standard/contract documents.

 

To unsubscribe, reply using "remove me" as the subject.

 

 

 


THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.

Subramani

unread,
Apr 9, 2010, 2:21:06 AM4/9/10
to material...@googlegroups.com
Dear Pradip,
 
Thank you very much for this detailed explanation. Yes, this would help individual companies to develop their own qualification procedure/guidelines.
 
Regards,
Subramani.
 