Can we use S355J2+N instead of ASTM A36

750 views
Skip to first unread message

Lalit Malla

unread,
Feb 27, 2017, 12:21:00 AM2/27/17
to Materials & Welding
Dear All,
Can we use S355J2+N plate instead of ASTM A36 plate for pipe support fabrication. In my opinion, S355J2+N is higher grade steel but will there be any problem with client acceptance ?
Your immediate response shall be highly appreciated. Thanks

Dinesh Somwanshi

unread,
Feb 27, 2017, 1:18:47 AM2/27/17
to materials-welding
Dear ,

Generally S 355J2 is not getting accepted, If available you  go with s275 grade,as listed in ASME 9, P1G1.

*DINESH VITTHAL SOMWANSHI*

*BACHELOR IN MECHANICAL ENGINEER*

*AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL,*
*API 570 - Piping Inspector,** AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3*
*NDT II -UT , RT , MT , PT, VT*
00919881344135
Skype = dinesh570_1

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e3de2f7-9b2d-43fb-a3ad-1c2be2431662%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

muthu barathi

unread,
Feb 27, 2017, 2:30:32 AM2/27/17
to material...@googlegroups.com


Dear Sir,


Very well you can use S355 J2 instead of A36. But the price difference would be more and same time written confirmation shall be obtained from the client.


Thanking You.

With Warm Regards,

Muthu Barathi P.
Mobile : +9184695933

Sent from RediffmailNG on Android

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrXw7TjPbGe-zKeuJEB0...@mail.gmail.com.

rudolf saldanha

unread,
Feb 27, 2017, 5:03:56 AM2/27/17
to material...@googlegroups.com, Lalit Malla

Hi S355 J2+N is much than A36, and your client is likely to accept your substitution

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

anthony chundal

unread,
Feb 27, 2017, 5:03:56 AM2/27/17
to material...@googlegroups.com
S355J2 material is not assigned with any P or Group nos, so in this case you cannot use the same, please advice what is your pipe material,  however in any case if you would like to use S355J2 you will have to qualify welding procedure as this is unassigned material. for A36 it is Pno-1 & Group no-1 which you can use without any issue.

Thanks & Regards,
Anthony.

On Mon, Feb 27, 2017 at 9:12 AM, Lalit Malla <lalit...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (lalit...@gmail.com) Add cleanup rule | More info

Dear All,
Can we use S355J2+N plate instead of ASTM A36 plate for pipe support fabrication. In my opinion, S355J2+N is higher grade steel but will there be any problem with client acceptance ?
Your immediate response shall be highly appreciated. Thanks

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

Suresh

unread,
Feb 27, 2017, 6:49:39 AM2/27/17
to material...@googlegroups.com
Hi 

You can use S355J2+N instead of A 36 unless like anthony specified, welding requirements because these materials are not in the assigned list .

Please pay attention on this ...However Client may exempt .



For more options, visit https://groups.google.com/d/optout.



--
Thanks  & Best Regards,

Suresh Paidi


 
Reply all