Change in welding progression is an essential variable as per API 1104.
Hence it is to be written separately and not together with slash (/).
Regards,
PARAG PANSARE
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a9d67ddb-c321-4f55-9247-7ccd9219d722%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Dear Mr. Parag,
Thank you very much. But the issue is the progression reversal had been done on the same material (x70) and same sizes in the PQRS but with different processes. In this case can I write WPS with different progressions for the hot pass seperately.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHB_ypDPyRWcawsowz8E68%2BNwz4gseBsrV7Vf2UZDzaVFsjR%3Dg%40mail.gmail.com.
Dear Mr. Chandrasekhar,
The welding process and progression both are essential variables, so you cannot write or club it together.
So in short for your each WPS you need to separately have only one qualified PQR.