Dear All,

I have a doubt from ASME Sec. IX as mentioned below , please clarify.

Welding Process : SMAW
Electrode used in PQR : E7018-1 (Kiswel)
Toughness Test : Applicable 

So as per Table (QW-253) - QW 404.12 is supplementary essential variable 

Electrode available Now : E7018-1 H4 (Oerlikon) & this has to be used in production now.

Suggest whether the manufacturer of welding consumable can be changed  with same electrode classification or new PQR has to be Qualified.

José Juan Jiménez Alejandro

unread,
Aug 18, 2020, 12:15:08 AM8/18/20
to material...@googlegroups.com
image.png

I consider that you should not do a new PQR since both electrodes are the same F number.
Regards!.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABLAf1LU2rQ%2BjYBXZp7NyefwaONeHqSH8gxn%3D3NYD5LK%2Bt1Qog%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SUMMIT MÉXICO - TPI

https://www.linkedin.com/in/summit-m%C3%A9xico-tpi-760047137/

Móvil +52 1 812 352 4606

Skype: jjjimeneza





harenath jha

unread,
Aug 18, 2020, 12:15:08 AM8/18/20
to material...@googlegroups.com
No new qualifications is required

ViNo Varughese

unread,
Aug 18, 2020, 12:15:09 AM8/18/20
to material...@googlegroups.com
You can proceed and no new PQR to be qualified.

Thanks & Regards
VV, Qatar


james gerald

unread,
Aug 18, 2020, 12:52:13 AM8/18/20
to material...@googlegroups.com
Only when you use an G classification electrode/Filler, Trade name is a supplementary essential variable. In your case change in Trade name will not affect & no need to qualify new PQR. WPS shall reflect the electrode/Filler with optional designator to be used in production

Thanks & Regards

J.Gerald Jayakumar




Gowtham Rajendran

unread,
Aug 18, 2020, 12:52:14 AM8/18/20
to material...@googlegroups.com
Thanks everyone one for your reply.