Dear Ahmad ,
The main difference between LTCS and Carbon manganese steel is the percentage of manganese , silicon and nickel which is pretty high in LTCS. LTCS weldability is similar to CS except it may require preheat , PWHT , hardness check as it mostly operates at low temp . You can use low hydrogen electrode ( E7018 ) and ER70S6 . Check for heat treatment and impact toughness requirements as per your project specification and do the necessary with your PQR .
Thanks
TDK Yokesh
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Regards,
Muhammad Babur Khan Lashari
Sr. QA/QC Inspector
(CSWIP 3.1 / CWI II From PWI)
Khaled Juffli Industial Company
Mob: + 966 56 2179280 / 58 2774568
PAK : + 92 334 6186285
Skype: babur.lashari
E-Mail: babur...@kjgroup.com
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BLU180-W7604117595E96ED7C220169EFB0%40phx.gbl.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1dff4f26-85ba-4a9d-a731-d037ac27bea3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.