Dear Experts ,

We intend to use SA 516 GR 70 plate - (thickness ranging from  55mm to 100 mm)  for   steam boiler application.
We are getting plates with Niobium content of 0.04 %.
As per SA 20   corresponding table ,the maximum limit for Nb  is 0.02 %
How ever , in the notes of the said Table  the Nb can be increased
What is effect of increase,  in Nb element on boiler drum shell rolling and  welding


Kannayeram Gnanapandithan

unread,
Dec 1, 2015, 12:08:12 AM12/1/15
to materials-welding
it will increase strength, inhibitors fine grains

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/05cb8aec-9be2-45e2-8d97-57c1b2dae3b7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages