Dear Experts,

I have a 80 mm dia pipe. I have done its wet chemical analysis according to IS228. The result shows as below,

C - 0.06
Si - 0.55
Mn - 0.45
P - 0.024
S - 0.023

I checked standard IS 1239. As per this standard, the chemical composition should be (all max), C - 0.2, Mn - 1.3, S&P - 0.04%.

My question is, can I say my pipe is IS 1239 pipe?

Please suggest what grade is my pipe?

Thank you.

Sincerely,
Abdulkadar

prem_nautiyal26

unread,
Sep 1, 2015, 5:22:27 AM9/1/15
to materials-welding
Hi

Unless you carry out chemical and mechanical testing how you can certify any material ?

Why don't you ask the lab which has done the chemical analysis to confirm the material grade composition please ?

Regards

Prem Nautiyal



Sent from Samsung Mobile
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ef3fedae-c74f-45ea-943f-2a10ab38ffd8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Alan Denney

unread,
Sep 1, 2015, 9:07:12 AM9/1/15
to material...@googlegroups.com

Jim Price

unread,
Sep 1, 2015, 9:19:59 AM9/1/15
to material...@googlegroups.com

If you have the material Certificate of Compliance from the mill yes.

If you want to verify the material then this should be for your information only.

Be very careful trying to recertify material.

By doing so you could be assuming liability.

 

Best Regard,

 

Jim Price | Welding Engineer, CWI

Direct:  320.7463439 |

jimp...@polarcorp.com

cid:image001.jpg@01D0E005.E9837830

 

 

 

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Kadir godil
Sent: Tuesday, September 01, 2015 3:55 AM
To: Materials & Welding
Subject: [MW:23378] DN 80 Carbon steel pipe

 

Dear Experts,

--

Kadir godil

unread,
Sep 2, 2015, 1:03:47 AM9/2/15
to material...@googlegroups.com
Thank you Alan, Jim & Prem,

It was a long ago used pipe. corroded so was examining it.  as a part of it, i analyzed the chemical composition. I was wondering, in IS 1239 there is no Si specification and this analysis shows it has Si content. That is why I was confused what grade should I call him.

thank you.