Difference between PTAW & PAW Processes

158 views
Skip to first unread message

Ilkin Hasanov

unread,
Jun 5, 2020, 1:26:20 AM6/5/20
to material...@googlegroups.com
Hi All,

Could you please advise what is different between PTAW & PAW Processes?



BR,
Ilkin Hasanov.

Yahoo Mail

unread,
Jun 5, 2020, 2:41:38 AM6/5/20
to material...@googlegroups.com

Types of Plasma ARC Welding 

The two modes of operation for the plasma welding process are the non-transferred arc and the transferred arc.

1) Transferred PAW

The transferred PAW method uses direct polarity DC current. And in this method, the tungsten electrode can                         be allied to the –ve terminal and the metal can be allied to the +ve terminal. The arc produces among tungsten                electrode as well as work portion. In this kind of method, both arc and plasma moved toward the work portion,                  which will enhance the heating capacity of the method. This type of PAW can be used to join solid / thick sheets.

2) Non-transferred PAW

The Non-transferred PAW method used direct polarity DC current and in this method the tungsten electrode can                    be connected to the –ve and the nozzle can be connected to the +ve pole. The arc generates among the nozzle                    as well as tungsten electrode within the torch, which will enhance the ionization of the gas within the torch.                          And the torch will transfer the ionized gas for further procedure. This type of PAW can be used to join thin sheets. 

The difference between these two modes of operation is shown below. The transferred arc mode is used for welding     metals. The gas tungsten arc process is shown for comparison.

Inline image
 Transferred and Non-transferred Plasma.

rgds,
C Sridhar
--------------------------------------------------------------------------------------------------------------------------------------------------------



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDZFkDNnqWYKYiUH_Pjj5tgo-TyysiH%2BXcLocwdWop086Q%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages