Dear expert, 
                      Can anyone explain hardness limit(value) of P-8(TP316,SS316L). 

Eg:- as you know that hardness vale of CS is 200BHN.

Macario Jr. Palola

unread,
Sep 16, 2024, 4:55:25 AM9/16/24
to material...@googlegroups.com
The hardness value of 316L stainless steel typically falls within the range of:

- Rockwell Hardness (HRB): 70-90
- Brinell Hardness (HB): Approximately 150-220

These values can vary based on the specific processing and treatment the steel has undergone.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACCHnjVGd7tiR8kA0-_G5y75nSwsN-2V%2BCECQHkmbKncBRafkg%40mail.gmail.com.

The information contained in this email is intended for use only by the recipient to whom or which this is addressed. Such information may be privileged, confidential, and/or proprietary subject to the GMEC Email Disclaimer. Moreover, as we value your privacy, we will handle and safeguard any personal data we receive in this email in accordance with our Privacy Notice.

Vishwas Keskar

unread,
Sep 16, 2024, 5:31:41 AM9/16/24
to material...@googlegroups.com
BASE METAL TYP 316 L 
Hardness limit - 22 HRC  maximum 


Sent from my iPhone

On 16 Sep 2024, at 2:25 PM, Macario Jr. Palola <macario...@gmec.ph> wrote:



kumar sumit

unread,
Sep 16, 2024, 5:31:41 AM9/16/24
to material...@googlegroups.com
Sir is there any reference standard plz quote. 

Srinivas Gundala

unread,
Sep 17, 2024, 12:17:37 AM9/17/24
to material...@googlegroups.com
Please follow NACE MR0175

Regards,



--
Thanks & Regards,
 
Srinivasrao.Gundala,

Please consider your environmental responsibility: before printing this e-mail, ask yourself whether you need a hard copy!
Reply all
Reply to author
Forward
0 new messages