PWHT requirement _ASME B31.8

220 views
Skip to first unread message

Manikandan J

unread,
Oct 24, 2022, 11:51:03 PM10/24/22
to material...@googlegroups.com
Dear Experts,

We have a Weld joint between Pipe to Hub as per sketch.

Run Pipe Thickness : 25.4 + 3 mm Cladding
Hub Thickness         : 31.8 + 3 mm Cladding    
Job Type : Weld joint in Piping
Code  : ASME B31.8-2020 Edn
image.png

Question 1 : For PWHT whether we need to consider Run pipe Thickness or Hub Thickness?.

Question 2 : If Run Pipe is considered for PWHT whether it includes Cladding Thk also?

Question 2 : If Hub is considered for PWHT whether it includes Cladding Thk also ?

Need your Views on this.

Regards,
Manikandan



james gerald

unread,
Oct 25, 2022, 11:29:13 PM10/25/22
to material...@googlegroups.com


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635


On Tuesday, 25 October, 2022 at 07:50:57 am GMT+4, Manikandan J <mechm...@gmail.com> wrote:


Dear Experts,

We have a Weld joint between Pipe to Hub as per sketch.

Run Pipe Thickness : 25.4 + 3 mm Cladding
Hub Thickness         : 31.8 + 3 mm Cladding    
Job Type : Weld joint in Piping
Code  : ASME B31.8-2020 Edn
image.png

Question 1 : For PWHT whether we need to consider Run pipe Thickness or Hub Thickness?. For set-in (Stub-in) connection, thickness of run Pipe and for set-on (Stub-on) connections, thickness of Header

Question 2 : If Run Pipe is considered for PWHT whether it includes Cladding Thk also? No

Question 2 : If Hub is considered for PWHT whether it includes Cladding Thk also ? No

Need your Views on this.

Regards,
Manikandan



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmORWERxzqJE4TfY58CzZxLA7J290D6Gqd1MV89zn%2BLVtA%40mail.gmail.com.

Mohd Siraj

unread,
Oct 29, 2022, 5:04:19 AM10/29/22
to Materials & Welding
whats material?

Manikandan J

unread,
Oct 29, 2022, 5:54:55 AM10/29/22
to material...@googlegroups.com
Material

Pipe : API 5L X60
Hub : A694 Gr.F60

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages