Dear Experts,

Can any body please tell me if there is any difference between ISO 10474 Vs EN 10204

Regards
G.Mohanraj

Prakash Gotimukul

unread,
Jul 2, 2018, 10:20:41 PM7/2/18
to materials-welding
One is a std published by EN and another by Iso. If you read carefully they are similar. But be careful with year of publication. EN is revised more regularly, so there may be differences.

Rgds.
Prakash G  AIS

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Kristian Lund Jepsen

unread,
Jul 2, 2018, 10:20:41 PM7/2/18
to material...@googlegroups.com

The main difference is that EN 10204 is harmonized to the European Pressure Equipment Directive, and material certificates for materials for pressure equipment to be CE marked to that directive need to be in accordance with EN 10204.

EN 10204 refers to another EN-standard giving instructions on what should be stated in the certificates.

 

Kind regards

Kristian

--