I have a query regarding welder qualification details as following. 
I have a WPS and PQR qualified as per ISO standard. 
can I qualify welders as per ASME sec 9 with that WPS or I have to follow EN ISO 9606-1 ?
Kindly advise. 

Thanks & Regards
Ritesh kr. Singh

venkateswara reddy Desireddy

unread,
Apr 6, 2024, 1:40:38 PMApr 6
to material...@googlegroups.com
Better to go with ISO


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-id5ypCk6_d6AnnJwGP4mLZ%2BeDxLs-s8OWZE6%2BARF8NZg%40mail.gmail.com.

madheswaran s

unread,
Apr 7, 2024, 11:51:43 AMApr 7
to material...@googlegroups.com
Go with Bs en ISO 9606-1 only . 