DIFFERENCE BETWEEN WROUGHT FITTINGS AND FORGED FITTINGS

15,842 views
Skip to first unread message

hemant

unread,
Oct 15, 2012, 11:59:29 PM10/15/12
to material...@googlegroups.com, Hardik Pandya

Dear All,

Can u explain me difference between wrought fittings and forged fittings? Can I use SA 182 instead of SA 403 or vies versa ? pls reply with code reference or technical reason.

 

Thanks,  

 

HEMANT SUTHAR

QA/QC

CEPL-SILVASSA

9712973092

 

sevak hiren

unread,
Oct 20, 2012, 9:59:25 AM10/20/12
to material...@googlegroups.com
Dear Concern,

Please refer following para of SA-182

 

5.4 The material shall be forged as close as practicable to the specified shape and size. Except for flanges of any type, forged or rolled bar may be used without additional hot working for small cylindrically shaped parts within the limits defined by Specification A 234/A 234M for low alloy steels and martensitic stainless steels and Specification A 403/A 403M for austenitic and ferritic-austenitic stainless steels. Elbows, return bends, tees, and header tees shall not be machined directly from bar stock.

 

5.5 Except as provided for in 5.4, the finished product shall be a forging as defined in the Terminology section of Specification A 788.


I suggest to use forged product instead of wrought product.


Definition of steel forging


The product of a substantially compressive plastic working operation that consolidates the material and produces the desired shape. The plastic working may be performed by a hammer, press, forging machine, ring rolling machine, or forging rolls, and must deform the material to produce an essentially wrought structure.



Definition of wrought fitting


Fittings made of pipe, tubing, plate or forgings by Forming process or Forging or shaping operations may be performed by hammering, pressing, piercing, extruding,upsetting, rolling, bending, fusion welding, machining, or by a combination of two or more of these operations.


The comparision between wrought product & forged product is as follow.


1) Wrought steel is less likely to be used in high-tension applications and it may be harder and more brittle than forged steel.


2) Forged steel is more durable in certain applications because, although it begins life as a casting as well, it is hammer forged using large hydraulic hammers that force the atoms and molecules of the steel into alignment as they hit it. Wrought steel does not undergo this same process, which makes forged steel harder and less likely to crack when struck. Striking tools and axes are often made of forged steel because they are used to hit things, and the brittle nature of a cast steel would lead them to breaking rapidly if they were not forged.


3) Forged steel may be more fine grained, in part because of the hammer-forging process.


Regards



--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 