RE: [MW:9569] P number grouping for IS 2062 material

2,666 views
Skip to first unread message

Bathula Raghuram (Mumbai - PIPING)

unread,
Sep 23, 2011, 6:40:03 AM9/23/11
to material...@googlegroups.com

IS2062 has been included in ASME BPV Sec IX 2011 addenda under P number 1 Group number 1 for all the three grades (i.e. A,B,C)

 

 

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Monday, January 31, 2011 9:12 AM
To: 'material...@googlegroups.com'
Subject: RE: [MW:9569] P1 no Range

 

IS 2062 is an unlisted material

SS 410 will under P number 6 ( refer table QW/QB 422)

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of puneet takiar
Sent: Sunday, January 30, 2011 8:04 PM
To: material...@googlegroups.com
Subject: Re: [MW:9565] P1 no Range

 

Hello!

Can anybody tell me in which P. no IS 2062 grade A and SS 410 will fall and how to search in ASME sex IX table.

Regards, 



Message has been deleted

Dominic Pereira

unread,
Nov 18, 2014, 2:48:12 AM11/18/14
to material...@googlegroups.com, r.ba...@ticb.com
Helloo All
can anyone let me know if IS:2041 is also included in P number group of ASME SectionIX.
If yes pls send me a snap shot of the same.

Regards
Dominic

hwj...@tce.co.in

unread,
Nov 18, 2014, 3:45:33 AM11/18/14
to material...@googlegroups.com, material...@googlegroups.com, r.ba...@ticb.com

Kindly note that IS 2062 is no  longer used for piping related work. See the 2011 version.







your truly
H W JOSHI
ENGINEER MECHANICAL
TATA CONSULTING ENGINEERS LTD
MUMBAI - 400 083
TEL : 022 61148409



Dominic Pereira <dominic.a...@gmail.com>
Sent by: material...@googlegroups.com

11/18/2014 01:55 PM


To
material...@googlegroups.com
cc
r.ba...@ticb.com
Subject
Re: [MW:22282] P number grouping for IS 2062 material





Helloo All
can anyone let me know if IS:2041 is also included in P number group of ASME SectionIX.
If yes pls send me a snap shot of the same.

Regards
Dominic

On Friday, September 23, 2011 4:10:03 PM UTC+5:30, Bathula Raghuram (Mumbai - PIPING) wrote:

IS2062 has been included in ASME BPV Sec IX 2011 addenda under P number 1 Group number 1 for all the three grades (i.e. A,B,C)

 

 

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)


Sent:
Monday, January 31, 2011 9:12 AM
To:
'

material...@googlegroups.com'


Subject:
RE: [MW:9569] P1 no Range

IS 2062 is an unlisted material

SS 410 will under P number 6 ( refer table QW/QB 422)

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of puneet takiar
Sent:
Sunday, January 30, 2011 8:04 PM
To:
material...@googlegroups.com
Subject:
Re: [MW:9565] P1 no Range

 

Hello!

Can anybody tell me in which P. no IS 2062 grade A and SS 410 will fall and how to search in ASME sex IX table.

Regards,


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.


----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------

Kanagaraj Ramasamy

unread,
Aug 4, 2016, 8:40:57 AM8/4/16
to Materials & Welding, R.Ba...@ticb.com
Could anyone provide thermal conductivity of IS2062 material for various temperatures?

DRNath

unread,
May 24, 2017, 6:30:52 AM5/24/17
to Materials & Welding
Dear Experts, Please share reference in ASME Section IX for p & g numbers for IS 2062 E350 gr. A, B, C materials if UNS no. is unknown
Reply all
Reply to author
Forward
0 new messages