Interpass Temp. Max
32 views
Skip to first unread message
P NAVEEN
unread,
May 29, 2024, 12:44:21 AM
May 29
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Hii,
What will be max Interpass temp of E 250 Br material in SMAW process.
Thanks
CHINTUKUMAR GANDHI
unread,
May 30, 2024, 10:13:45 AM
May 30
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
You can consider it 315º C as per API RP-582 considering ASME Sec. IX P-No. 1 material.
Thanks
C. R. GANDHI
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com
.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/9f7f2618-5371-4558-88cf-9ab14a5d1988n%40googlegroups.com
.
Reply all
Reply to author
Forward
0 new messages