Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash
image.png

Can we provide the weld 

---------- Forwarded message ---------
From: Chiranjeevi A <chiranjee...@gmail.com>
Date: Fri, 12 Jul, 2019, 11:10 PM
Subject: Pipe shoe support_urgent
To: <material...@googlegroups.com>


Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash
image.png

harenath jha

unread,
Jul 13, 2019, 12:33:26 PM7/13/19
to material...@googlegroups.com
Please provide weld relief as per drawing. That's required

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0y03Qz6CxAPDB2qPk4_6EFXcfAuOSr4yu2cuLJf352%3D4g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Eng.Mahmoud kamel

unread,
Jul 13, 2019, 12:33:30 PM7/13/19
to material...@googlegroups.com
Yes you can , 

first get company engineering approval , and modify detail DEG 






Best regards
mahmoud
00201009087426


From: material...@googlegroups.com <material...@googlegroups.com> on behalf of Chiranjeevi A <chiranjee...@gmail.com>
Sent: Saturday, July 13, 2019 7:19 AM
To: material...@googlegroups.com
Subject: [MW:29824] Fwd: Pipe shoe support_urgent
 

harenath jha

unread,
Jul 15, 2019, 1:34:53 AM7/15/19
to material...@googlegroups.com
Whenever we have designed such type of support we always provide this, this will serve two purpose
1. To avoid weld over weld and 
2. This will act as a escape route of welding gas. 

Mohamed Muneeb

unread,
Jul 15, 2019, 1:34:53 AM7/15/19
to materials-welding
Yes , very comprehensive design with innovative come back for typical subject of weld clashing with shoe.

As said seek the designers advise / approval.

Srinivasulu Kalasapati

unread,
Jul 15, 2019, 1:34:53 AM7/15/19
to material...@googlegroups.com
Yes you can provide, prior take engineering approval, also, band slots and relief slots to be shown as dotted lines in front view, is the line insulated


On Saturday, July 13, 2019, Chiranjeevi A <chiranjee...@gmail.com> wrote:
Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash
image.png

Can we provide the weld 

---------- Forwarded message ---------
From: Chiranjeevi A <chiranjee...@gmail.com>
Date: Fri, 12 Jul, 2019, 11:10 PM
Subject: Pipe shoe support_urgent
To: <materials-welding@googlegroups.com>


Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash
image.png

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.


--
Ohm Guru Namasivaya

Bathula AnilKumar

unread,
Jul 15, 2019, 1:34:53 AM7/15/19
to material...@googlegroups.com
Yes We Can provide, mouse hole shall be 25 mm away from weld on both sides

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


--

Thanks and Regards,
Bathula Anil Kumar
SC:- 1873,
Phone number:- 99351283, 94350267

atul khatri

unread,
Jul 15, 2019, 5:07:40 AM7/15/19
to material...@googlegroups.com
HI,
Graphics shows that its a normal sliding support (i believe that line size is not higher than 10"). This weld relief will not impose any issue. These things generally happens and such notch does serve the purpose.
So just go ahead but with prior approval.

--

Srinivasulu Kalasapati

unread,
Jul 16, 2019, 11:19:41 PM7/16/19
to material...@googlegroups.com
Dear all,

Several experts said that provide, but with prior engg approval, actually what needs to be reviewed by engg for approval....

Its a sliding shoe, the web strength doesn't effect much, intact on welding inside the relief area w.r.t pipe increases the strength...  the web doesn't buckle down...

So its just dwg approval and no need of verifying the structural integrity.....



On Monday, July 15, 2019, atul khatri <atul....@gmail.com> wrote:
HI,
Graphics shows that its a normal sliding support (i believe that line size is not higher than 10"). This weld relief will not impose any issue. These things generally happens and such notch does serve the purpose.
So just go ahead but with prior approval.

On Sat, Jul 13, 2019 at 8:46 PM Chiranjeevi A <chiranjee...@gmail.com> wrote:
Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash
image.png

Can we provide the weld 

---------- Forwarded message ---------
From: Chiranjeevi A <chiranjee...@gmail.com>
Date: Fri, 12 Jul, 2019, 11:10 PM
Subject: Pipe shoe support_urgent
To: <materials-welding@googlegroups.com>


Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash
image.png

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


--
Ohm Guru Namasivaya

George Dilintas

unread,
Jul 17, 2019, 12:24:06 PM7/17/19
to material...@googlegroups.com
on my opinion support without saddle is a bad design. You get high stress concentration at the pipe


For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

atul khatri

unread,
Jul 17, 2019, 12:24:06 PM7/17/19
to material...@googlegroups.com
This is the weld which transfers load from pipe to shoe plate.
Any decrease in weld area  (due to notch) actually may reduce the strength of shoe.
Generally shoe plates thickness are kept same for a range of pipe size to avoid fabrication of different shoes based on pipe size and thickness. For example , a plate thickness of 10 mm may be used to manufacture these T type shoes for pipe size 4"-10" having schedule or thickness in range of 6- 12.7 mm. 
So in your case if the pipe size is coming lesser than the maximum pipe size in that range than you can proceed.  


To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


--
Ohm Guru Namasivaya

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages