Portable PMI machine

54 views
Skip to first unread message

Biplab Pal

unread,
Jan 17, 2016, 1:18:06 AM1/17/16
to materials-welding
Dear Friends,

Can you please guide me if there is any portable PMI machine(fit for use any condition) available  which can measure Carbon content.
I will appreciate if you send me the Catalog (If any).

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

pgoswami

unread,
Jan 17, 2016, 9:16:08 AM1/17/16
to material...@googlegroups.com

Biplab,

 

Please take a look at these products .They’re quite reliable and not so difficult to carry at worksite (if one carries small canister of purge gas). You need to talk to the manufacturer and ask for a site demo if required. Your other option is to ask directly the NDE service providers.

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist & Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

 

http://www.oxford-instruments.com/products/spectrometers/optical-emission-spectroscopy


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg0C2Mf68MEi9H8KuxU9K6EF%2BcvZskpeCSa19UYUrfop8w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Shashank Vagal

unread,
Jan 18, 2016, 7:09:21 AM1/18/16
to material...@googlegroups.com
No.
 
BR,
Shashank C Vagal 




From: pgoswami <pgos...@quickclic.net>
To: material...@googlegroups.com
Sent: Sunday, 17 January 2016 7:45 PM
Subject: [MW:24116] RE: 24115] Portable PMI machine

Biplab Pal

unread,
Jan 18, 2016, 7:09:42 AM1/18/16
to materials-welding

chinmayee4 .

unread,
Jan 22, 2016, 2:01:13 AM1/22/16
to material...@googlegroups.com
Yes, There is a machine called   XMATE 2000.  you will find internet.  There are some XRF models . 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg0C2Mf68MEi9H8KuxU9K6EF%2BcvZskpeCSa19UYUrfop8w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks with Regards


Sivayya
Competent Person 
D. NO. 13-32/15, F. No. 107, 
SVLN Paradise -1, NAD Layout, 
Chinamushidivada,
Opp. Sujatha Nagar. 
Visakhapatnam - 530051
Mobile : 9346868777

Mohd Azam

unread,
Jan 22, 2016, 7:23:22 AM1/22/16
to material...@googlegroups.com

Its available in market, Niton series machine is having that capacity…Just go to the web site or supplier, will provide all relevant information

 

Thanks & Regards,

Mohd. Azam

Doha- Qatar


Reply all