PWHT for A276 Ty.410 + Stellite-6 (ERCoCr-A)

27 views
Skip to first unread message

Brajendra Singh

unread,
Jun 4, 2018, 7:42:59 AM6/4/18
to Materials & Welding
Dear Experts,

Please suggest what is the recommended temp for PWHT of Following Combination.

Process: PTAW (Plasma transfered Arc)
Material thickness: 30 mm
MOC: A276 Ty.410
Overlay type: Hard-facing overlay by ERCoCr-A

thanks in advance.

Brajendra Patel
Welding Engineer
Mob:+917057406907

Sankaran Sp

unread,
Jun 5, 2018, 1:15:54 AM6/5/18
to material...@googlegroups.com
Dear Mr.Brajendra Patel,

while hard facing of Er CoCrA on  410 type material by any process( ie: PTA or GTAW), Tempering is not required, PWHT only required. Since tempering will affect the quality of CoCrA hard face, hence PWHT is enough and furnace cooling to Room temp is best industrial practice.        

Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore,India


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Kannayeram Gnanapandithan

unread,
Jun 5, 2018, 1:59:41 AM6/5/18
to materials-welding
why do not give temp for SR/PWHT, he asking that only.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Mon, Jun 4, 2018 at 7:24 PM, 'Sankaran Sp' via Materials & Welding <material...@googlegroups.com> wrote:
Dear Mr.Brajendra Patel,

while hard facing of Er CoCrA on  410 type material by any process( ie: PTA or GTAW), Tempering is not required, PWHT only required. Since tempering will affect the quality of CoCrA hard face, hence PWHT is enough and furnace cooling to Room temp is best industrial practice.        

Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore,India


On Monday, 4 June, 2018, 5:13:02 PM IST, Brajendra Singh <brajen...@gmail.com> wrote:


Dear Experts,

Please suggest what is the recommended temp for PWHT of Following Combination.

Process: PTAW (Plasma transfered Arc)
Material thickness: 30 mm
MOC: A276 Ty.410
Overlay type: Hard-facing overlay by ERCoCr-A

thanks in advance.

Brajendra Patel
Welding Engineer
Mob:+917057406907

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages